Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 100 kJ/m² @Temperature -30.0 °C |
47.6 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® 500RS PC (Europe-Africa-Middle East) LEXAN 500RS is a medium viscosity, glass reinforced, flame retardant grade. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² @Temperature -30.0 °C |
47.6 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® 503RS PC (Europe-Africa-Middle East) LEXAN 503RS is a medium viscosity, glass reinforced, flame retardant grade UV stabilized grade. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX MS002 PP (Asia Pacific) LNP* Faradex* MS002 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Unnotched (ISO) | >= 100 kJ/m² | >= 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DL003 PC (Europe-Africa-Middle East) LNP* Lubricomp* DL003 is a compound based on Polycarbonate resin containing PTFE. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² - NB | 47.6 ft-lb/in² - NB | Average value: 109 kJ/m² Grade Count:6 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Glass Filled". Each property range of values reported is minimum .. |
|||
Izod Impact, Unnotched (ISO) | >= 100 kJ/m² | >= 47.6 ft-lb/in² | 80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® EXRL1061 PC (Asia Pacific) Transparent Polycarbonate in natural color. Excellent processability, super high flow. |
|||
Izod Impact, Unnotched (ISO) | >= 100 kJ/m² @Temperature -30.0 °C |
>= 47.6 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1U |
SABIC Innovative Plastics Lexan® EXRL1061 PC (Asia Pacific) Transparent Polycarbonate in natural color. Excellent processability, super high flow. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² - NB | 47.6 ft-lb/in² - NB | Average value: 100 kJ/m² Grade Count:10 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² - NB | 47.6 ft-lb/in² - NB | Average value: 105 kJ/m² Grade Count:4 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP FARADEX MS002 PP (Europe-Africa-Middle East) LNP* Faradex* MS002 is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing 20% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP PFP36 PA 6 LNP* LUBRICOMP* PFL36 is a compound based on Nylon 6 resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | ISO 180/1eU |
Solvay TECHNYLSTARâ„¢ SX 216 V60 PA6, 60% glass filled, Conditioned Description: TECHNYL STAR TM Polyamide reinforced with 60% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North America Product Applicat.. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | ISO 180/1eU |
Solvay TECHNYLSTARâ„¢ SX 218 V50 PA6, 50% glass filled, Conditioned Description: TECHNYLSTARâ„¢ SX 218 V50 is based on a patented high flow polyamide 6 resin (Technylstar), heat stabilized, reinforced with 50% of glass fiber, for injection molding. This product i.. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | ISO 180/1eU |
Solvay TECHNYLSTARâ„¢ SX 218 V60 Black Z PA6, 60% glass filled, Conditioned Description: TECHNYLSTAR Polyamide reinforced with 60% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt. Available in: Asia Pacific, Europe and No.. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp ZP001 PPE+PS (Europe-Africa-Middle East) LNP* LUBRICOMP* ZP001 is a compound based on PPE+PS Blend resin containing PTFE, Silicone. Added features include Internally Lubricated.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² @Temperature -30.0 °C |
47.6 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics Valox® 325FC PBT (Europe-Africa-Middle East) Commercial, VALOX 325FC is compliant with food contact regulations. VALOX 325FC is a general purpose, unreinforced PBT injection moulding resin which contains internal mold release. This new 325FC g.. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² @Temperature -40.0 °C |
47.6 ft-lb/in² @Temperature -40.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Europe-Africa-Middle East) LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Asia Pacific) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOTUF PK003ER PA 6 (Europe-Africa-Middle East) High Impact Nylon 6 compound containing Mineral, Impact Modifier. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RV00ASXP PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00ASXP is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | DIN 53453 |
Wico Plast Wicotal 500 Acetal ApplicationsInjection moldingAll information provided by Wico Plast, Warenhandelsges. mbH |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | DAM; ISO 180/1U |
DuPont Performance Polymers Zytel® 73G30L NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Polyamide 6Zytel 73G30L NC010 is a 30% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 50%RH; ISO 180/1U |
DuPont Performance Polymers Zytel® 8018HS NC010 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 8018HS NC010 is a 14% glass reinforced heat stabilized toughened polyamide 66 resin.Information provided by DuPont Performance Polym.. |
|||
Izod Impact, Unnotched (ISO) | >= 100 kJ/m² | >= 47.6 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Staramide PX06093 PA6, Impact Modified, Injection Molded Staramide PX06093 is an UV Stabilized, Impact Modified Polyamide 6 Injection Molding Resin (also known as P1000HI020UVL)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | >= 100 kJ/m² @Temperature -30.0 - -30.0 °C |
>= 47.6 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 100 kJ/m² Grade Count:1 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP DL003E PC LNP LUBRICOMP* DL003E is a compound based on Polycarbonate resin containing 15% PTFE. Added features of this material include: Easy Molding, Internally Lubricated |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² @Temperature 23.0 °C |
47.6 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Verton RV00CEU PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00CEU is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, UV Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP VERTON RV00CEXP PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00CE is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding. |
|||
Izod Impact, Unnotched (ISO) | 100 kJ/m² | 47.6 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics Xenoy® X5630 PC+PET (Europe-Africa-Middle East) Mineral filled PC/PET blend with high heat dimensional stability, low shrinkage and low CTE, especially for painted applications |