Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 180 MPa | 26100 psi | |
Lehmann & Voss LUVOCOM® 1105-8160 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Tensile Stress | 180 MPa | 26100 psi | |
Lehmann & Voss LUVOCOM® 1105-8161 PEEK, with carbon fiber, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; low thermal coefficient of expansion.Dynamic stressed parts at high m.. |
|||
Tensile Stress | 180 MPa | 26100 psi | |
Lehmann & Voss LUVOCOM® 1105-8168 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.High chemical resista.. |
|||
Tensile Stress | 180 MPa | 26100 psi | |
Lehmann & Voss LUVOCOM® 1301/CF/20 PPS, linear, with carbon fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |
|||
Tensile Stress | 180 MPa | 26100 psi | |
Lehmann & Voss LUVOCOM® 1301-7178 PPS, linear, with glass fiber Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.High continuous use and heat distortion temperature. .. |
|||
Tensile Stress | 180 MPa | 26100 psi | |
Lehmann & Voss LUVOCOM® 1301-7449 PPS, linear, with carbon fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Improved friction and wear behaviour. Emergency runni.. |
|||
Tensile Stress | 180 MPa | 26100 psi | |
Lehmann & Voss LUVOCOM® 1-7332/GY Polyamide 66, with carbon fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh.. |
|||
Tensile Stress | 180 MPa | 26100 psi | |
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15 Polyamide 66, with glass fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Tensile Stress | 180 MPa | 26100 psi | |
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/SI/2-2 Polyamide 66, with glass fiber, PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Tensile Stress | 180 MPa | 26100 psi | |
Lehmann & Voss LUVOCOM® 1104-7452 Polyether ketone, with glass fiber, easy flowing Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Improved fatigue properties.Thermic, mechanic and chemical highly str.. |
|||
Tensile Stress | 180 MPa | 26100 psi | |
Lehmann & Voss LUVOCOM® 1105/GF/40/BK-1 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Tensile Stress | 180 MPa | 26100 psi | |
Lehmann & Voss LUVOCOM® 1105-8402 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension.. |
|||
Tensile Stress | 180 MPa | 26100 psi | |
Lehmann & Voss LUVOCOM® 1106-8374 Polyether imide, with carbon fiber and PTFE Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig.. |
|||
Tensile Stress | 180 MPa | 26100 psi | |
Lehmann & Voss LUVOCOM® 1114-0717 PAEK, with carbon fiber and PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Electrically conduct.. |
|||
Tensile Stress | 180 MPa | 26100 psi | |
Lehmann & Voss LUVOCOM® 1105-0858 PEEK, with glass fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.High dimensionally stable precision parts, high continuous use tempera.. |
|||
Tensile Stress | 180 MPa | 26100 psi | ISO 527-2 |
Solvay Specialty Polymers Ryton® R-4-02XT Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4XT and R-4-02XT 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength with good electrical properties and outstanding chemical resistance, even.. |
|||
Tensile Stress | 180 MPa | 26100 psi | |
Lehmann & Voss LUVOCOM® 1105-7241-1 PEEK, with glass fiber and PTFE Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.dynamic stressChemical and hydrolysis resistance pa.. |
|||
Tensile Stress | 180 MPa | 26100 psi | |
Lehmann & Voss LUVOCOM® 1-7233-1 Polyamide 66, with glass fiber, PTFE, lubricant modified, silicone-free Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, .. |