Mechanical Properties Metric English Comments
Tensile Strength at Break 156 MPa
22600 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics EXTEM XH2315 TPI Resin
Extem XH2315 Resin
Tensile Strength at Break 156 MPa
22600 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics EXTEM XH2315 TPI Resin (Asia Pacific)
Extem XH2315 Resin
Tensile Strength at Break 156 MPa
22600 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics EXTEM XH2315 TPI Resin (Europe-Africa-Middle East)
Extem XH2315 Resin
Tensile Strength at Break 156 MPa
22600 psi
ISO 527
Gharda Chemicals GATONE™ PEEK, 30% Glass Reinforced  (discontinued **)
GATONE™ PEEK grades with glass fiber reinforcements ranging from 10- 40 % are available in natural or desired colors. Custom made grades can be developed to meet specific requirements.CHARACTERISTI..
Tensile Strength at Break 156 MPa
22600 psi
ISO 527
Nilit FRIANYL A63 HS-GV50 Nylon 6.6 for injection molding, 50% glass fiber reinforced
Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Tensile Strength at Break 156 MPa
22600 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP EX07305 PEI (Asia Pacific)
Polyetherimide reinforced with Glass fiber and PTFE for use in Burn-in Test Sockets (BiTS) Application
Tensile Strength at Break 156 MPa
22600 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP RFG16 PA 66 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RFG16 is a compound based on PA 66 resin containing Glass Fiber, Graphite. Added features include: Internally Lubricated.
Tensile Strength at Break 156 MPa
22600 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP LF005 PEEK
LNP* THERMOCOMP* LF005 is a compound based on Polyetheretherketone resin containing 25% Glass Fiber.
Tensile Strength at Break 156 MPa
22600 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP LF005 PEEK (Asia Pacific)
LNP* Thermocomp* LF005 is a compound based on Polyetheretherketone resin containing Glass Fiber.
Tensile Strength at Break 156 MPa
22600 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP PX85100 PA 6
LNP* THERMOCOMP* PX85100 is a compound based on Nylon 6 resin containing Proprietary Filler(s).
Tensile Strength at Break 156 MPa
22600 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP PX85100 PA 6
LNP* THERMOCOMP* PX85100 is a compound based on Nylon 6 resin containing Proprietary Filler(s).
Tensile Strength at Break 156 MPa
22600 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP QF007 PA 6/10
LNP* THERMOCOMP* QF007 is a compound based on Nylon 6/10 resin containing 35% Glass Fiber.
Tensile Strength at Break 156 MPa
22600 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF004 PA 66
LNP THERMOCOMP* RF004 is a compound based on Nylon 66 resin containing 20% Glass Fiber.
Tensile Strength at Break 156 MPa
22600 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF004H PA 66
LNP* THERMOCOMP* RF004H is a compound based on Nylon 66 containing 20% Glass Fiber. Added feature of this grade is: Healthcare.
Tensile Strength at Break 156 MPa
22600 psi
ASTM D638
SABIC Innovative Plastics LNP THERMOCOMP RF004XXD PA 66
LNP THERMOCOMP* RF004XXD is a compound based on Nylon 66 resin containing 20% Glass Fiber.
Tensile Strength at Break 156 MPa
22600 psi
Type I, 5 mm/min; ASTM D638
SABIC Innovative Plastics LNP THERMOTUF IX02582 PA6.12
LNP* Thermotuf* IX02582 is a compound based on Nylon 6/12 resin containing Proprietary Filler(s). Added features of this material include: High Impact.
Tensile Strength at Break 156 MPa

@Temperature -40.0 °C
22600 psi

@Temperature -40.0 °F
ISO Data
BASF Ultramid® A3EG3 15% Glass Filled PA66 (Dry)
Ultramid A3EG3 is a 15% glass fiber reinforced injection molding PA66 grade. It conforms to FDA requirements of 21 CFR 177.1500.
Tensile Strength at Break 156 MPa
22600 psi
ISO 527
SABIC Innovative Plastics LNP VERTON NV008E PC/ABS (Asia Pacific)
LNP* Verton* NV008E is a compound based on PC/ABS resin containing Long Glass Fiber. Added features of this material include: Easy Molding.
Tensile Strength at Break 156 MPa
22600 psi
ISO 527
SABIC Innovative Plastics LNP VERTON NV008E PC+ABS
LNP* VERTON* NV008E is a compound based on PC+ABS resin containing 40% Long Glass Fiber. Added features of this material include: Easy Molding. Structural.