Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 758 MPa | 110000 psi | |
Performance Alloys MoldStar® 21 (PAS 21) Bronze Mold Alloy Description: MoldStar® 21 bronze alloy provides good bearing qualities and resistance to wear, abrasion, fatigue, deformation and corrosion.Applications: Lifter BladesSlidesGibsWear PlatesEjector S.. |
|||
Tensile Strength at Break | 758 MPa | 110000 psi | 4140 Steel butt joint |
Lucas-Milhaupt EASY FLO 45 Silver Based Cadmium-Bearing Filler Metal Applications: Easy-Flo 45 is very versatile and can be used successfully on nearly all nickel, iron and copper base alloys. In certain instances, special fluxes, may be required to obtain good wet.. |
|||
Tensile Strength at Break | 758 MPa | 110000 psi | Hard |
Special Metals MONEL® 404 Copper-Nickel Alloy Data provided by California Fine Wire and the manufacturer, Special Metals. |
|||
Tensile Strength at Break | 760 - 890 MPa | 110000 - 129000 psi | |
Schmolz + Bickenbach UGICHROM 4507 Duplex Chrome Plated Bar Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef.. |
|||
Tensile Strength at Break | 758 MPa | 110000 psi | Hard |
California Fine Wire Nickel Alloy 99 All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 758 MPa | 110000 psi | Hard |
California Fine Wire Nickel Alloy 99 Nickel Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 758 MPa | 110000 psi | Stress relieved |
California Fine Wire Nico Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | 758 MPa | 110000 psi | Stress relieved |
California Fine Wire Stablohm 825 Nickel Chromium Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Tensile Strength at Break | >= 758 MPa | >= 110000 psi | |
Carlson C 625 Nickel-Chromium-Molybdenum Alloy General DescriptionCarlson Alloy C 625 is a nickel-chromium-molybdenum alloy that combines high strength and oxidation resistance with excellent corrosion resistance. C 625 exhibits exceptional fat.. |
|||
Tensile Strength at Break | 760 MPa | 110000 psi | |
Bisalloy Steels BisPlate 70 Thickness >80-100 mm Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness. Can be welded with minimal preheat and has excellent low temperat.. |
|||
Tensile Strength at Break | 760 MPa | 110000 psi | |
Bisalloy Steels BisPlate 70 Thickness 16-80 mm Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness. Can be welded with minimal preheat and has excellent low temperat.. |
|||
Tensile Strength at Break | 760 MPa | 110000 psi | |
Bisalloy Steels BisPlate 70 Thickness 5 - Low carbon, low alloy, high strength structural steel exhibiting excellent cold formability and low temperature fracture toughness. Can be welded with minimal preheat and has excellent low temperat.. |