California Fine Wire Nico Copper Nickel Resistance Wire

Category Metal , Electronic/Magnetic Alloy , Nonferrous Metal , Copper Alloy , Nickel Alloy
Manufacturer California Fine Wire
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF California Fine Wire Nico Copper Nickel Resistance Wire.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 8.91 g/cc
0.322 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 414 MPa
60000 psi
Annealed
758 MPa
110000 psi
Stress relieved
931 MPa
135000 psi
Hard
Thermal Properties Metric English Comments
CTE, linear 14.9 µm/m-°C

@Temperature 20.0 °C
8.28 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.393 J/g-°C

@Temperature 20.0 °C
0.0939 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 21.0 W/m-K
146 BTU-in/hr-ft²-°F
Melting Point 1210 °C
2210 °F
Maximum Service Temperature, Air 1000 °C
1830 °F
Operating Temperature
Component Elements Properties Metric English Comments
Copper, Cu 55 %
55 %
Nickel, Ni 45 %
45 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000489 ohm-cm
0.0000489 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic None
Temperature Coefficient of Resistance ±0.00002 ohms/ohm-°C
0-100°C
Thermal EMF vs. Copper -0.045