Material Notes:
All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 7.11 g/cc
0.257 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 621 MPa
90000 psi
Annealed
758 MPa
110000 psi
Stress relieved
896 MPa
130000 psi
Hard
Thermal Properties Metric English Comments
CTE, linear 11.4 µm/m-°C

@Temperature 20.0 °C
6.33 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.460 J/g-°C

@Temperature 20.0 °C
0.110 BTU/lb-°F

@Temperature 68.0 °F
Melting Point 1510 °C
2750 °F
Maximum Service Temperature, Air 316 °C
601 °F
Operating Temperature
Component Elements Properties Metric English Comments
Aluminum, Al 2.5 %
2.5 %
as balance
Chromium, Cr 20 %
20 %
Iron, Fe 2.5 %
2.5 %
as balance
Nickel, Ni 75 %
75 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.000137 ohm-cm
0.000137 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic Strong
Temperature Coefficient of Resistance 0.00002 ohms/ohm-°C
0-100°C
Thermal EMF vs. Copper -0.004