Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 70.0 MPa | 10200 psi | ISO 527 |
Nilit FRIANYL B63 KLZ Nylon 6 for injection molding Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 163R PC (Europe-Africa-Middle East) LEXAN 163R is a medium viscosity multi purpose U.V. stabilized grade and contains a release agent to ensure easy processing. LEXAN 163R is available in transparent, translucent and opaque colours. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 201R PC (Europe-Africa-Middle East) LEXAN 201R is a high viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.8 mm approved. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXD103R PC (Asia Pacific) FXD103R is a Light Diffusion effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color Package may affect propert.. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXD143R PC (Europe-Africa-Middle East) LEXAN FXD143R is a transparent/translucent medium viscosity grade for light diffusion effects. UV-stabilized. The color package may affect performance. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXE144R PC (Europe-Africa-Middle East) LEXAN FXE144R is a transparent/translucent medium viscosity grade for special effect colours with a fluorescent appearance. The grade is suitable for food contact applications. The colour package ma.. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC (Asia Pacific) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® ML3987 PC (Europe-Africa-Middle East) LEXAN ML3987 is a highly UV stabilised grade which has been developed as a coextrusion product exhibiting a low plate out behaviour and improved outdoor weathering of LEXAN sheet.This data was suppl.. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® OQ4120R PC (Europe-Africa-Middle East) Optical grade with UV cut-off up to 400 nm, greater optical purity than standard grades. For needs of sunglass and sunvisor markets. MFR of 25. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® SLX1431D PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® SLX2431T PC Copolymer Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® SLX2471T PC Copolymer (Europe-Africa-Middle East) Medium viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | ISO.527 DN.53455 |
Polimersan Plastics POLIPOM® (POM) POLIPOM® is a plastic which is manufactured by the polymerization of formaldehyde. Its high proportional crystallized structure of the oxygen and methyl groups inside, provides it high proportional.. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® HP6 PC Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mo.. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® SLX1231D PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Strength at Break | 70.0 MPa @Temperature 80.0 °C |
10200 psi @Temperature 176 °F |
50 mm/min, 1A; ISO 527 |
SABIC Innovative Plastics SABIC STAMAX 30YM243 PP SABIC® STAMAX 30YM243 is a 30% long glass fiber reinforced UV stabilized polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMD.. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | ISO 527-1/-2 |
Unitika A3130 PA6, 35% Mineral Reinforced, Dry Information provided by Unitika Ltd. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | ISO 527-93 |
Wellman EcoLon® MR1660-BK1 Nylon 66, 40% Mineral Reinforced All information provided by Wellman Engineered Resins. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | ISO 527-93 |
Wellman Wellamid® NY1820-BK1(PTFE) Lubricated, Heat Stabilized Nylon 66 Description: Lubricated, Heat Stabilized Nylon 66Information provided by Wellman. |
|||
Tensile Strength at Break | 70.0 - 72.0 MPa | 10200 - 10400 psi | DIN 53455 |
Zell-Metall Engineering Plastics Zellamid 1100 MO at 50% RH Improved sliding and self-lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.Color: blackApplications: For conveyor screws |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | ISO 527-1/-2 |
DSM Akulon® K224-HG3 (Cond.) 15% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® AG-30 LF 15 PA66-(GF+Z)45 Product description: Grilon AG-30 LF 15 black 9832 is a heat stabilized, normal viscosity PA66 injection molding grade with 30% glass fibers and 15% of a combination of PTFE and silicone. Grilon AG-.. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
Chi Mei Wonderlite® PC-122 Polycarbonate High Flow |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | 5 mm/min; ISO 527 |
Eurostar Starflam AFR682B1 PA66, Mineral Reinforced, Flame Retardant, Injection Molding Starflam AFR682B1 is a Flame Retardant, Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | ISO 527 |
Eurotec® Tecomid® NB30 MF30 BK001 HS PA6, 30% mineral reinforced, heat stabilized, black Information provided by Eurotec® |
|||
Tensile Strength at Break | 70.0 MPa @Temperature 160 - 175 °C, Time 1.80e+7 sec |
10200 psi @Temperature 320 - 347 °F, Time 5000 hour |
5 [mm/min], 50% Loss of Tensile Strength; ICE 216 |
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Dry, 15% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | ISO 527 |
Eurotec® Tecomid® NB40 NL FA50 PA6, unfilled, flame retardant - halogen free, natural Information provided by Eurotec® |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | ISO 527 |
Eurotec® Tecomid® NB40 NL FN70 PA6, unfilled, flame retardant - halogen free (RoHS compliant), natural Information provided by Eurotec® |
|||
Tensile Strength at Break | 70.0 MPa | 10200 psi | ISO 527-93 |
Wellman Wellamid® 22LH-WBK Unfilled Nylon 66 Description: Unfilled Nylon 66Information provided by Wellman. |