Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched = 5.34 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.60 - 5.34 J/cm
3.00 - 10.0 ft-lb/in
Average value: 2.38 J/cm Grade Count:11
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Izod Impact, Unnotched 2.14 - 5.34 J/cm
4.00 - 10.0 ft-lb/in
Average value: 2.96 J/cm Grade Count:10
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Izod Impact, Unnotched 2.14 - 5.34 J/cm
4.00 - 10.0 ft-lb/in
Average value: 3.01 J/cm Grade Count:26
Overview of materials for Polycarbonate/ABS Alloy, NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, NCG Fiber Filled". Each property range of values reported is minimum and maximu..
Izod Impact, Unnotched 1.76 - 5.34 J/cm
3.30 - 10.0 ft-lb/in
Average value: 3.17 J/cm Grade Count:28
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max..
Izod Impact, Unnotched 3.20 - 5.34 J/cm
6.00 - 10.0 ft-lb/in
Average value: 3.83 J/cm Grade Count:6
Overview of materials for Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 50% Glass Fiber Filler". Specific grades with glass content between 45%..
Izod Impact, Unnotched 3.20 - 5.34 J/cm
6.00 - 10.0 ft-lb/in
Average value: 3.74 J/cm Grade Count:9
Overview of materials for Nylon 66, Mineral Filled, NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, NCG Fiber Filled". Each property range of values reported is minimum and maxim..
Izod Impact, Unnotched 2.67 - 5.34 J/cm
5.00 - 10.0 ft-lb/in
ASTM D256
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug..
Izod Impact, Unnotched 2.67 - 5.34 J/cm
5.00 - 10.0 ft-lb/in
Average value: 4.10 J/cm Grade Count:7
Overview of materials for Polyetherimide (PEI), Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Aramid Fiber Filled". Each property range of values reported is minimum and maximum valu..
Izod Impact, Unnotched 2.67 - 5.34 J/cm
5.00 - 10.0 ft-lb/in
Average value: 4.08 J/cm Grade Count:10
Overview of materials for Polyetherimide (PEI), Nickel Coated Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "PEI, NCG Filled". Each property range of values reported is minimum and maximum values of appropriate Ma..
Izod Impact, Unnotched 3.20 - 5.34 J/cm
6.00 - 10.0 ft-lb/in
Average value: 4.76 J/cm Grade Count:7
Overview of materials for Polyphenylene Ether, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu..
Izod Impact, Unnotched 1.60 - 5.34 J/cm
3.00 - 10.0 ft-lb/in
Average value: 4.19 J/cm Grade Count:15
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min..
Izod Impact, Unnotched 4.27 - 5.34 J/cm
8.00 - 10.0 ft-lb/in
Average value: 4.85 J/cm Grade Count:6
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m..
Izod Impact, Unnotched 0.481 - 5.34 J/cm
0.900 - 10.0 ft-lb/in
Average value: 4.30 J/cm Grade Count:14
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Izod Impact, Unnotched 3.36 - 5.34 J/cm
6.29 - 10.0 ft-lb/in
Average value: 4.04 J/cm Grade Count:5
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and ..
Izod Impact, Unnotched 2.67 - 5.34 J/cm
5.00 - 10.0 ft-lb/in
Average value: 3.63 J/cm Grade Count:5
Overview of materials for Polypropylene with Glass Fiber + PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with Glass Fiber + PTFE". Each property range of values reported is minimum and maximum va..
Izod Impact, Unnotched 0.400 - 5.34 J/cm
0.749 - 10.0 ft-lb/in
Average value: 3.00 J/cm Grade Count:18
Overview of materials for Polypropylene, Wood Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Wood Filled". Each property range of values reported is minimum and maximum values of app..
Izod Impact, Unnotched 1.60 - 5.34 J/cm
3.00 - 10.0 ft-lb/in
Average value: 2.76 J/cm Grade Count:7
Overview of materials for Polypropylene with 40% Mica Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are..
Copyright © lookpolymers.com All Rights Reserved