Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.80 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
8.99 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256 |
PolyOne Maxxam™ PPC-10G Nat Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 1100-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-15 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 3101-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 3101-15 is a fiberglass reinforced thermoset bulk molding compound for electrical circuit breakers, switchgear and other applications where fire retardance is required.Key features and .. |
|||
Izod Impact, Unnotched | 4.80 J/cm @Temperature -30.0 °C |
8.99 ft-lb/in @Temperature -22.0 °F |
ASTM D4812 |
SABIC Innovative Plastics Cycoloy® C4220 PC+ABS PC+ABS Blend with 20% Glass Reinforce. High heat resistance; Excellent balance strength/rigidity; Good impact/appearance. |
|||
Izod Impact, Unnotched | 4.80 J/cm @Thickness 3.18 mm |
8.99 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Emi-X® OC-1008 LEX Polyphenylene Sulfide, Carbon Fiber Reinforcement
(discontinued **) Features: Radio Frequency Shielding, Electromagnetic Shielding, Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data .. |
|||
Izod Impact, Unnotched | 4.80 - 5.90 J/cm | 8.99 - 11.1 ft-lb/in | Average value: 5.33 J/cm Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), Stainless Fiber, EMI This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Stainless Fiber, EMI". Each property range of values reported is minimum and maximum va.. |
|||
Izod Impact, Unnotched | 4.80 J/cm @Thickness 3.18 mm |
8.99 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® JF-1004 EM M BK905 Polyethersulfone, Milled Glass Fiber
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® FL933 PC Various weight reductions at 0.250"" wall. 30% GR. Superior flexural strength and modulus; good tensile strength. UV-stabilized. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2100 PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
Izod Impact, Unnotched | 4.80 J/cm @Temperature 23.0 °C |
8.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem 2100N PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2100R PEI 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2100R PEI (Asia Pacific) 10% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2200 PEI 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. NSF 51 listing, WRAS certification in recognized colors. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2200R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2210R PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM HU2200 PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DEL13EXC PC (Asia Pacific) LNP* STAT-KON* DEL13EXC is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 4521 PBT VALOX 4521 is a high flow, 20% glass reinforced flame retardant PBT injection moulding resin. Applications: electrical applications |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 4521 PBT (Asia Pacific) 19.5% glass reinforced PBT. High flow, flame retardant. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 8032U PBT+PET (Europe-Africa-Middle East) VALOX 8032U is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. Applications: appliance housings, door handles, mirror brackets. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Asia Pacific) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON EX01696C PEI LNP* STAT-KON* EX01696C is a compound based on Polyetherimide resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
Izod Impact, Unnotched | 4.80 J/cm @Temperature 23.0 °C |
8.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp RF005 PA 66 (Asia Pacific) LNP* Thermocomp* RF005 is a compound based on Nylon 66 resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched | 4.80 J/cm @Temperature 23.0 °C |
8.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp KCL36 Acetal Copoly LNP* Lubricomp* KCL36 is a compound based on Acetal Copolymer resin containing PTFE, Carbon Fiber. Added features of this material include: Internally Lubricated, Electrically Conductive.This data .. |
|||
Izod Impact, Unnotched | 4.80 J/cm @Temperature 23.0 °C |
8.99 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D4812 |
DuPont Performance Polymers Minlon® FE6190 BK086 Nylon 66 Minlon® FE6190 BK086 is a 36% mineral/glass reinforced, heat stabilized, black polyamide resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Unnotched | 4.80 - 5.20 J/cm @Temperature 23.0 °C |
8.99 - 9.74 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds ART 0699 Rigid PVC, Atoxic for General Purpose Bottles suitable for containing oils |
|||
Izod Impact, Unnotched | 4.80 J/cm | 8.99 ft-lb/in | ASTM Test |
BASF Ultramid® 8262G HS BK-102 7/13% Glass/Mineral Filled PA6 (Dry) Ultramid 8262G HS BK-102 is a heat stabilized, pigmented black, 20% glass and mineral reinforced PA6 injection molding compound resulting in a balance of engineering properties with excellent dimens.. |
|||
Izod Impact, Unnotched | 4.80 - 5.20 J/cm @Temperature 23.0 °C |
8.99 - 9.74 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RI 548/H Rigid PVC, Antishock Injection Molding Electric antishock fittings |
|||
Izod Impact, Unnotched | 4.80 J/cm @Temperature -40.0 °C |
8.99 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Adell RR-19 Polypropylene Copolymer; 43% Glass Reinforced, High Impact Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 4.80 J/cm @Temperature -40.0 °C |
8.99 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Adell RR-39 Polypropylene Copolymer; 43% Glass Reinforced, High Impact Data provided by Adell Plastics, Inc. |