Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 13.35 J/cm | 25.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP COLORCOMP EX12304C PEI (Asia Pacific) LNP* Colorcomp* EX12304C is an unfilled polyetherimide clean compound with extremely high level of cleanliness for the most demanding application. This compound is manufactured using LNP CCS technol.. |
|||
Izod Impact, Unnotched | >= 13.35 J/cm | >= 25.01 ft-lb/in | ASTM D256 |
Ineos H00G-00 Polypropylene Homopolymer A polypropylene homopolymer produced by Ineos utilizing catalyst technology. This material meets the Food and Drug Administration requirements of 21CFR 177.1520. Homopolymer H00G-00 meets certain .. |
|||
Izod Impact, Unnotched | 13.35 J/cm | 25.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 1000F PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer.. |
|||
Izod Impact, Unnotched | 13.35 J/cm @Temperature 23.0 °C |
25.01 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem 1000M PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 13.35 J/cm @Temperature 23.0 °C |
25.01 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem 1000M PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched | 13.35 J/cm | 25.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 1000R PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
Izod Impact, Unnotched | 13.35 J/cm @Temperature 23.0 °C |
25.01 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem 1000RV PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Afr.. |
|||
Izod Impact, Unnotched | 13.35 J/cm | 25.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 1010 PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer be .. |
|||
Izod Impact, Unnotched | 13.35 J/cm @Temperature 23.0 °C |
25.01 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem 1010A PEI Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 13.35 J/cm @Temperature 23.0 °C |
25.01 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem 1010A PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched | 13.35 J/cm @Temperature 23.0 °C |
25.01 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem 1010A PEI (Europe-Africa-Middle East) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched | 13.35 J/cm | 25.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 1010F PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant, NSF 51 listing. Effective June 2007, this grade will no longer b.. |
|||
Izod Impact, Unnotched | 13.35 J/cm | 25.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 1010K PEI Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Izod Impact, Unnotched | 13.35 J/cm @Temperature 23.0 °C |
25.01 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem 1010KM PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched | 13.35 J/cm @Temperature 23.0 °C |
25.01 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem 1010RV PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Americas r.. |
|||
Izod Impact, Unnotched | 13.35 J/cm | 25.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 1010TC PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing. |
|||
Izod Impact, Unnotched | 13.35 J/cm @Temperature 23.0 °C |
25.01 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem 1010V PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
Izod Impact, Unnotched | 13.35 J/cm @Temperature 23.0 °C |
25.01 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem 1010V PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
Izod Impact, Unnotched | 13.35 J/cm @Temperature 23.0 °C |
25.01 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem 1010V PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing.This data wa.. |
|||
Izod Impact, Unnotched | 13.35 J/cm | 25.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 9011 PEI Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. Improved processability for Fiber extrusion. |
|||
Izod Impact, Unnotched | 13.35 J/cm | 25.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM HU1000 PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Izod Impact, Unnotched | 13.35 J/cm | 25.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM HU1000 PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI).. |
|||
Izod Impact, Unnotched | 13.35 J/cm | 25.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM HU1000E PEI Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (.. |
|||
Izod Impact, Unnotched | 13.35 J/cm | 25.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM HU1000E PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (.. |
|||
Izod Impact, Unnotched | 13.35 J/cm | 25.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM HU1010 PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),.. |
|||
Izod Impact, Unnotched | 13.35 J/cm | 25.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 1000E PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. US FDA and EU Food Contact compliant. |
|||
Izod Impact, Unnotched | 13.35 J/cm | 25.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM AUT200 PEI Transparent high flow Polyetherimide (Tg 217C). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperat.. |
|||
Izod Impact, Unnotched | 13.35 J/cm @Temperature 23.0 °C |
25.01 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D4812 |
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66
(Unverified Data**) Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide.. |
|||
Izod Impact, Unnotched | 13.35 J/cm | 25.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 1000E PEI Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. US FDA and EU Food Contact compliant, NSF 51 Listing. Effective June, 2007 this grade will no longer.. |
|||
Izod Impact, Unnotched | 13.35 J/cm | 25.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 1010M PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. |