Mechanical Properties Metric English Comments
Charpy Impact Unnotched 2.00 - 3.00 J/cm²

@Temperature -30.0 - -30.0 °C
9.52 - 14.3 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 2.41 J/cm² Grade Count:8
Overview of materials for Polyetheretherketone, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu..
Charpy Impact Unnotched 2.50 - 3.00 J/cm²
11.9 - 14.3 ft-lb/in²
Average value: 2.70 J/cm² Grade Count:3
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and ..
Charpy Impact Unnotched 3.00 - 3.00 J/cm²

@Temperature -30.0 - -30.0 °C
14.3 - 14.3 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 3.00 J/cm² Grade Count:1
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 20% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 20% Glass Reinforced". Each property range of values reported is minimum and maximum values..
Charpy Impact Unnotched 3.00 - 3.00 J/cm²

@Temperature -30.0 - -30.0 °C
14.3 - 14.3 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 3.00 J/cm² Grade Count:1
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and ..
Charpy Impact Unnotched 2.20 - 3.00 J/cm²

@Temperature -30.0 - 30.0 °C
10.5 - 14.3 ft-lb/in²

@Temperature -22.0 - 86.0 °F
Average value: 2.52 J/cm² Grade Count:6
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an..
Charpy Impact Unnotched 0.800 - 3.00 J/cm²
3.81 - 14.3 ft-lb/in²
Average value: 2.27 J/cm² Grade Count:3
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi..
Charpy Impact Unnotched 0.700 - 3.00 J/cm²
3.33 - 14.3 ft-lb/in²
Average value: 1.97 J/cm² Grade Count:23
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini..
Charpy Impact Unnotched 1.80 - 3.00 J/cm²
8.57 - 14.3 ft-lb/in²
ISO 179
Bulk Molding Compounds tetra-DUR F 4401 Bulk Molding Compound
UL-licensed, general purpose productTypical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prot..
Charpy Impact Unnotched 1.80 - 3.00 J/cm²
8.57 - 14.3 ft-lb/in²
ISO 179
Bulk Molding Compounds tetra-DUR L 4305 Bulk Molding Compound
UL-licensed. Anchor wave-isolation.Typical Applications - Requiring mechanical strength, abrasion resistance, dimensional stability, electrical insulation, electrostatic dissipation (explosion prote..
Charpy Impact Unnotched 2.00 - 3.00 J/cm²
9.52 - 14.3 ft-lb/in²
Average value: 2.50 J/cm² Grade Count:3
Overview of materials for Acetal Copolymer + Glass/PTFE
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of ..
Charpy Impact Unnotched 2.00 - 3.00 J/cm²

@Temperature -20.0 - -20.0 °C
9.52 - 14.3 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 2.45 J/cm² Grade Count:8
Overview of materials for Polypropylene with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are in..
Copyright © lookpolymers.com All Rights Reserved