Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | >= 6.00 J/cm² @Temperature 23.0 °C |
>= 28.6 ft-lb/in² @Temperature 73.4 °F |
Injection Molded; ISO 179 |
PolyOne Bergamid™ B70 G30 grey VN7445CF Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | |
Polycasa Acryl® KR 2015/1 Acrylic, Impact Grade Medium-impact grade with very good flow behavior, especially mechanically stressed parts with long flow paths; e.g. strip light diffusers. Can be extruded into thin tubes, sheet and film.Data was c.. |
|||
Charpy Impact Unnotched | 6.00 - 6.00 J/cm² @Temperature -30.0 - -30.0 °C |
28.6 - 28.6 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 6.00 J/cm² Grade Count:1 |
Overview of materials for Nylon 610, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1-7789/EG Polyamide 66, with carbon fiber, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Antistatic.High dimensi.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1-8357 Polyamide 66, with carbon fiber and glass fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; impact resistance.Electrically conductive, suitable for continuous dischar.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 20-7847 Polyphthalamide, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | |
LATI Latiohm 66-05 PD01 G/20 PA66, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | ISO 179/1EA-1993 |
Solvay Technyl® B 50H1 Nylon 66/6, Flame Retardant, EH0 Flame retardant copolyamide 66/6, unreinforced, heat stabilized, for injection molding.This phosphorus and halogen free flame retardant grade, UL 94 VO (0.4 mm), offers excellent filling qualities a.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | ISO Data, Low Temp |
Styron Magnum™ 358HP ABS, High Heat MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-30 HM PA6-GF30 Product description: Grilon BG-30 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 30% glass fibers. Grilon BG-30 HM has the following important prop.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BGM-30 X PA6-(GF+MD)30 Product description: Grilon BGM-30 X is a heat stabilized PA 6 injection molding grade with a 30 % reinforcement combination (mineral and glass fiber). Grilon BGM-30 X has the following important pr.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® TE250F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, Flame Retardant (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GVS 20/10 HWCP 20% Glass Fiber and 10% Glass Sphere Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 30.0 °C |
28.6 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® GVS-5H nat PA*-GF50 Product description: Grivory GVS-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 30.0 °C |
28.6 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® HT2V-45H PA6T/66-GF45 Grivory HT2V-45H is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation acc. to ISO: PA 6T/66 Acc. to AST.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® LV-3 X ESD black PA12-GF30 Grilamid LV-3 X ESD black is an antistatic Polyamide 12 for injection molding with 30% glass fiber reinforcement. Main attributes are: antistatic with resistivity < 106 Ohmgood fuel and zinc chlorid.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 30.0 °C |
28.6 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSG-30/4 W PA666-GF30 Product description: Grilon TSG-30/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4102 black 9238 PA*-CF30 Grivory XE 4102 is a 30% carbon fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewab.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 30.0 °C |
28.6 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 4102 black 9238 PA*-CF30 Grivory XE 4102 is a 30% carbon fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partially based on renewab.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® LBV-65H FWA black 9225 PA12-GF65 Product description: Grilamid LBV-65H FWA black 9225 is a 65% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features High stiffness combined.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® XE 5004 (BM-30/2 UV) PA666-MD30 Product description: Grilon XE 5004 is a normal viscosity PA6 injection molding grade with 30% mineral reinforcement, which is additionally UV stabilized. Grilon XE 5004 has the following important .. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
|
BASF Procom® GC40S 402 Polypropylene Uses: Electrical appliance housings (e.g. drills), components requiring high impact and temperature resistance, furniture frames.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature -30.0 °C |
28.6 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | Conditioned; ISO 179/IeU |
Addiplast Addinyl A2 ZG30 Nylon 66, 30% Glass Bead Glass bead reinforced, improved stiffness and dimensional stability, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | ISO 179/1eU |
BASF Ultradur® B 4406 G6 30% Glass Filled PBT Description: Is a PBT, flame-retardant injection-molding grades, with 30% glass fibers, for parts requiring enhanced fire resistance, e.g. plug-and-socket connectors, housings, coil formers and ligh.. |
|||
Charpy Impact Unnotched | 6.00 J/cm² @Temperature 23.0 °C |
28.6 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Lanxess Pocan® TS 3220 901510 PBT + PET, 20% Glass Fiber PBT+PET, 20% glass fibers, injection molding, impact modified, low tendency to warp, improved surface finish |
|||
Charpy Impact Unnotched | 6.00 J/cm² | 28.6 ft-lb/in² | ISO 179/1eU |
Pasargad Polymer Peyvand Pasamid 3P-L1130B Nylon 6, 30% Glass Fiber Reinforced Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Electrical PartsFastenerHousingInformation provided by Pasargad Polymer Peyvand Co |
|||
Charpy Impact Unnotched | 6.00 J/cm² - NB | 28.6 ft-lb/in² - NB | Average value: 14.6 J/cm² Grade Count:25 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |