Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | flatwise; ISO 179 1fU |
Lehmann & Voss LUVOCOM® 1105-8135/GN PEEK, unreinforced, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Especially suitable for medical parts, superheated steam sterilizable, hydrolysis resistan.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 50-8276 Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.High dimensionally stable precision parts, even at elevated te.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature -30.0 °C |
42.8 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Lustran® M203FC Standard impact strength, easy flowing, high gloss, BgVV and FDA quality for food contact. ,Property data per ISO test methods. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature -30.0 °C |
42.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 1/XCF/30 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 23.0 °C |
42.8 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Gromax CFG35-R113N1 Nylon 6 36% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | ISO Data, Low Temp |
Styron Magnum™ 9010 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 30.0 °C |
42.8 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® 2SV-30H nat PA610-GF30 Product Description: GRILAMID XE3976 natural 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mat.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BG-30 S FA PA6-GF30 Product description: Grilon BG-30 S FA is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 S FA has the following important properties: Excellent surface finishEasy .. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BG-30 S PA6-GF30 Product description: Grilon BG-30 S is a heat stabilized PA6 injection molding grade with 30% glass fibers. Grilon BG-30 S has the following important properties: Excellent surface finishEasy flowin.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® GV-5H black PA*-GF50 Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® GV-5H EF black 9915 PA*-GF50 Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® LV-50H FWA nat PA12-GF50 Product description: Grilamid LV-50H FWA natural is a 50 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® LVX-65H SST nat PA12-GF65 Product description: Grilamid LVX-65H SST natural is a 65% glass fiber reinforced, heat stabilized engineering thermoplastic based on polyamide 12 for complex structural parts with the following pro.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSG-35 PA666-GF35 Information provided by EMS Grivory |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature 30.0 °C |
42.8 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSG-50/4 W PA666-GF50 Product description: Grilon TSG-50/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | 50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 73G30HSL BK261 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK261 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 for injection molding. It has excellent surface app.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | 50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR BK083 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-50 S PA6-GF50 Product description: Grilon BG-50 S is a heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 S has the following important properties: High stiffnessExcellent surface fin.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | |
BASF Novolen® 1040 RC Polypropylene, Injection Molding Grade Injection moldingsData was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature -30.0 °C |
42.8 ft-lb/in² @Temperature -22.0 °F |
|
BASF Polystyrol® 456 F Impact Grade Polystyrene (Europe) Heat distortion resistant, good flowing grade for parts subjected to heat.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact Unnotched | 9.00 J/cm² @Temperature -30.0 °C |
42.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
BASF Ultramid® B3ZG6 30% Glass Filled PA6 (Dry) Ultramid B3ZG6 is an impact-modified, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | ISO 179/1eU |
BASF Ultramid® B3GK24 10/20% Glass Bead/Fiber Filled PA6 (Conditioned) Ultramid B3GK24 is 30% combined glass-fiber and glass bead injection molding PA6 grade for industrial articles having very high dimensional stability. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® MN201-G35 Nylon 66 Resin 35% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | dry; ISO 179/1eU |
EMS-Grivory Grivory® BG-50 FC PA6-GF50 Product description: Grilon BG-50 FC is a heat stabilized PA6 injection molding grade with 50% glass fibers. Grilon BG-50 FC has the following important properties: Short cycle timesExcellent surfac.. |
|||
Charpy Impact Unnotched | 9.00 J/cm² | 42.8 ft-lb/in² | conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BGZ-15/2 PA6-GF15 Product description: Grilon BGZ-15/2 is a heat stabilized and impact modified PA6 injection molding grade with 15% glass fibers. Grilon BGZ-15/2 has the following important properties: Good impact s.. |