Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 FRB 4 LS Polyamide 6, Halogen Free Flame Retardant, Light Stabilization FeaturesPA 6 for injection moulding with increased flammability resistance with non-halogen flame retardant. Determined for electrical purposes. Excellent flow of the material predetermines it for.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 OB Polyamide 6, Optically Brightened FeaturesPA 6 for injection moulding, optical brightened, for mouldings with high surface brightness, with increased toughness and tensile modulus in comparison with the basic type. The microcrystal.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6/66 GF 20 T 10 FRG 5 PA6/66, 20% glass fibre, flame retardant Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 66/6 T 30 TS PA66/6, 30% mineral filling FeaturesPA 66/PA 6 alloy with the content of 30 % chemically modified mineral filling. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat products, autom.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Polykemi AB POLYfill PP CIP15015 Polypropylene, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYfill PPH GF1020 Polypropylene Homopolymer, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYform POM C M270 Polyoxymethylene Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYshine PBT D223 GF10 FR PBT, Glass-Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB POLYshine PBT D234 GF30 FR PBT, Glass-Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
|
Radici Radilon® S HS (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 0.400 - 0.500 J/cm² @Temperature 23.0 °C |
1.90 - 2.38 ft-lb/in² @Temperature 73.4 °F |
Compression; ISO 179/ 1eA |
Raschig Group 2568 AMC Glass fiber-reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, heat resistant up to 500°C for short time - usable for s.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
PolyOne Bergamid™ A700 Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6/66 CF 30 PA6/66, 30% carbon fibre FeaturesPA 6/66 for injection moulding, chemically strengthened with 30% of carbon fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PPH T2040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYshine PBT D201 T20 PBT, Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 3-9230 KAR YU UV-Stabilized, 26% Mineral-Filled Compound Blend Of Polypropylene Homopolymer And Block-Copolymer INNOPOL® CS 3-9230 KAR YU is a yellow colored, UV-stabilized, 26% mineral-filled compound based on a blend of polypropylene homopolymer and block-copolymer.INNOPOL® CS 3-9230 KAR YU is develop.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
|
LATI Laramid G/15 PPA, 15% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Ultem 1100EF PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® VX7024 PBT (Europe-Africa-Middle East) VALOX VX7024 is a 12% mineral filled PBT injection moulding resin with excellent mechanical properties.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Styrolution Luran® S 777 K UV Black 56625 ASA Description: Easy flowing injection molding grade with good toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis BC142MO Polypropylene Copolymer BC142MO is a controlled rheology polypropylene heterophasic copolymer. It is characterized by high impact strength, good stiffness, excellent process ability, good flow properties and low warpage. .. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis BH345MO Polypropylene Copolymer BH345MO is a heterophasic copolymer. This grade is characterized by optimum combination of very high stiffness, good flow properties and good impact strength. and is designed for high speed injectio.. |
|||
Charpy Impact, Notched | 0.399 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
cond; ISO 179/1eA |
DSM Akulon® Ultraflow K-FHGM35 PA6-(GF+MD)40 15% Glass Reinforced, Heat Stabilized, High Flow |
|||
Charpy Impact, Notched | 0.399 J/cm² @Temperature -20.0 °C |
1.90 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
ExxonMobil AP3N Polypropylene Impact Copolymer Product Description: A medium impact copolymer resin designed for appliance applications requiring good stiffness and fast cycle time.Availability: Asia Pacific Features:Fast Molding CycleHigh Glos.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eA |
DSM Novamid® 3010SR NAT PA66 Easy Molding Grade |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
cond; ISO 179/1eA |
DSM Stanyl® TW341-J PA46 Heat Stabilized, Lubricated |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
ISO 179/eA |
Eurotec® Tecomid® NA40 NL XA 20 PA 6.6 unreinforced, UL94 V0 Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
DSM Akulon® K-FHGM24 (Dry) 30% Glass/Mineral Reinforced, Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DSM Akulon® K-FHGM24 (Dry) 30% Glass/Mineral Reinforced, Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Charpy Impact, Notched | 0.400 J/cm² @Temperature 23.0 °C |
1.90 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® VX5530 PBT (Europe-Africa-Middle East) VALOX VX5530 is a flame retarded, 15% glass fibre reinforced, 10% mineral filled PBT+PC blend with excellent low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |