Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.87 - 3.20 J/cm | 3.50 - 6.00 ft-lb/in | ASTM D265 |
Alcoa KAMA 3400 Super High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableMono-layer an.. |
|||
Izod Impact, Notched | 0.427 - 3.20 J/cm | 0.800 - 6.00 ft-lb/in | Average value: 0.931 J/cm Grade Count:15 |
Overview of materials for Liquid Crystal Polymer (LCP), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Carbon Fiber Filled". Each property range of values reported is minimum an.. |
|||
Izod Impact, Notched | 2.14 - 3.20 J/cm | 4.00 - 6.00 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 1201-10 Polyester SMC
(discontinued **) Premi-Glas® 1201-10 is a 10% glass reinforced thermoset Sheet Molding Compound designed for sinks, shower stall bases and wall applications. Key features and benefits are:Supports ANSI 124.2 and CS.. |
|||
Izod Impact, Notched | 2.14 - 3.20 J/cm | 4.00 - 6.00 ft-lb/in | ASTM D256 |
Mar-Bal MB1000-15 Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Izod Impact, Notched | 2.67 - 3.20 J/cm | 5.00 - 6.00 ft-lb/in | ASTM D256 |
Mar-Bal MB1000-PC Thermoset Polyester Composite Molding Compound A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.Mar-Bal standard grades can be injection, compression and transfer molded.Information pro.. |
|||
Izod Impact, Notched | 2.14 - 3.20 J/cm | 4.00 - 6.00 ft-lb/in | ASTM D256 |
Mar-Bal MB2000-10 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Izod Impact, Notched | 1.60 - 3.20 J/cm | 3.00 - 6.00 ft-lb/in | ASTM D256 |
ScanTube PVDF Tubing Information provided by ScanTube, Inc. |
|||
Izod Impact, Notched | 2.14 - 3.20 J/cm | 4.00 - 6.00 ft-lb/in | |
Bulk Molding Compounds BMC 1902 Mineral Filled Alkyd BMC 1902 molding compound is a mineral filled, glass-fiber-reinforced alkyd compound suitable for compression molding. It was developed primarily for applications requiring very good impact and flex.. |
|||
Izod Impact, Notched | 1.07 - 3.20 J/cm | 2.00 - 6.00 ft-lb/in | |
Bulk Molding Compounds BMC 310 Cosmetic and Appliance Grade Compound BMC 310 is a cosmetic and appliance grade material with superior heat and stain resistant properties. As with all other BMCI compounds, this Series can be supplied in logs, slugs or bulk.Typical app.. |
|||
Izod Impact, Notched | 1.07 - 3.20 J/cm | 2.00 - 6.00 ft-lb/in | |
Bulk Molding Compounds BMC 605LS Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605LS molding compound is a low-shrink, mineral filled, glass-fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good mol.. |
|||
Izod Impact, Notched | 2.14 - 3.20 J/cm | 4.00 - 6.00 ft-lb/in | |
Bulk Molding Compounds BMC 615 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 615 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. It is a high impact material produced in ext.. |
|||
Izod Impact, Notched | 1.60 - 3.20 J/cm | 3.00 - 6.00 ft-lb/in | |
Bulk Molding Compounds BMC A30 General Purpose Molding Compound BMC A30 is a general purpose molding compound with good dimensional stability. Due to the excellent flow and controlled reactivity, BMC A30 is well suited for injection, transfer or compression mol.. |
|||
Izod Impact, Notched | 1.60 - 3.20 J/cm | 3.00 - 6.00 ft-lb/in | |
Bulk Molding Compounds BMC A30-3021 General Purpose Molding Compound BMC A30-3021 is a low shrink, general purpose molding compound formulated for the lighting industry. A30-3021 is temperature stabilized for use in elevated temp. lighting applications. Due to the .. |
|||
Izod Impact, Notched | 1.07 - 3.20 J/cm | 2.00 - 6.00 ft-lb/in | |
Bulk Molding Compounds BMC 1000 Thermoset Polyester, Food Grade BMC 1000 is a general purpose, food contact grade, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding. As with all other BMC, Inc. compounds, .. |
|||
Izod Impact, Notched | 1.07 - 3.20 J/cm | 2.00 - 6.00 ft-lb/in | |
Bulk Molding Compounds BMC 605 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 605 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good moldability, medi.. |
|||
Izod Impact, Notched | 2.14 - 3.20 J/cm | 4.00 - 6.00 ft-lb/in | |
Bulk Molding Compounds BMC 8005 Polyester Molding Compound |
|||
Izod Impact, Notched | 2.67 - 3.20 J/cm | 5.00 - 6.00 ft-lb/in | |
Bulk Molding Compounds BMC SLC 2000 Glass Reinforced Polyester BMC SLC 2000 is a medium strength, low-cost, glass reinforced polyester compound with adjustable shrinkage. Ideal for circuit breakers, motor switch housings, fuse holders, brush holders, standoff i.. |
|||
Izod Impact, Notched | 0.427 - 3.20 J/cm | 0.800 - 6.00 ft-lb/in | Average value: 1.14 J/cm Grade Count:16 |
Overview of materials for Polypropylene, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Notched | 2.14 - 3.20 J/cm | 4.00 - 6.00 ft-lb/in | |
Bulk Molding Compounds BMC T70 Automotive Grade Molding compound BMC T70 is a low profile automotive grade molding compound specifically formulated for the vacuum metallization process. These compounds have excellent physical properties as well as superior adhes.. |