| Category | Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass and Mineral Filled BMC |
| Manufacturer | BMC - Bulk Molding Compounds Inc. |
| Trade Name | BMC |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Bulk Molding Compounds BMC 8005 Polyester Molding Compound.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 2.00 g/cc | 2.00 g/cc | |
| Water Absorption | <= 0.16 % | <= 0.16 % | 24 hours, 23°C |
| Linear Mold Shrinkage | <= 0.0010 cm/cm | <= 0.0010 in/in |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Barcol | 50 - 65 | 50 - 65 | |
| Tensile Strength, Ultimate | 48.3 - 62.1 MPa | 7000 - 9000 psi | |
| Flexural Strength | 138 - 172 MPa | 20000 - 25000 psi | |
| Compressive Strength | 172 - 207 MPa | 25000 - 30000 psi | |
| Izod Impact, Notched | 2.14 - 3.20 J/cm | 4.00 - 6.00 ft-lb/in |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | >= 260 °C | >= 500 °F | |
| Flammability, UL94 | HB | HB |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 15.2 - 16.9 kV/mm | 385 - 430 kV/in | Short Time |
| Arc Resistance | >= 180 sec | >= 180 sec |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Mold Temperature | 138 - 166 °C | 280 - 330 °F |