Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.500 - 1.20 J/cm | 0.937 - 2.25 ft-lb/in | Average value: 0.858 J/cm Grade Count:10 |
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Izod Impact, Notched | 0.370 - 1.20 J/cm | 0.693 - 2.25 ft-lb/in | Average value: 0.744 J/cm Grade Count:28 |
Overview of materials for Polycarbonate/ABS Alloy, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Carbon Fiber Filled". Each property range of values reported is minimum and max.. |
|||
Izod Impact, Notched | 1.00 - 1.20 J/cm | 1.87 - 2.25 ft-lb/in | ASTM D256 |
Loxim 140 01V0 Polycarbonate, 40% Glass Filled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 1.00 - 1.20 J/cm | 1.87 - 2.25 ft-lb/in | ASTM D256 |
Loxim 830 01 HBCC Polypropylene Compound 30% Chemically Coupled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.400 - 1.20 J/cm @Thickness 4.00 mm |
0.749 - 2.25 ft-lb/in @Thickness 0.157 in |
ASTM D256 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D.. |
|||
Izod Impact, Notched | 0.600 - 1.20 J/cm @Thickness 4.00 mm |
1.12 - 2.25 ft-lb/in @Thickness 0.157 in |
ASTM D256 |
Solvay Specialty Polymers Solef® 9007 Polyvinylidene Fluoride (PVDF) Solef® 9007 PVDF homopolymer has low viscosity and is used in film extrusion and injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 53... |
|||
Izod Impact, Notched | 0.700 - 1.20 J/cm | 1.31 - 2.25 ft-lb/in | Average value: 1.03 J/cm Grade Count:10 |
Overview of materials for Polyvinyl Dichloride (PVDC) This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap.. |
|||
Izod Impact, Notched | 0.300 - 1.20 J/cm @Temperature -30.0 - -30.0 °C |
0.562 - 2.25 ft-lb/in @Temperature -22.0 - -22.0 °F |
Average value: 0.567 J/cm Grade Count:122 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |