Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8310 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet Digital Materials™ DM_8320 Rigid Opaque Prototyping Polymer Primary material: VeroWhitePlusSecondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet VeroBlack FullCure870 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet VeroClear FullCure810 Information provided by Proto3000 for their protoyping engineering services. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256A |
Proto3000 WaterShed® XC 11122 Stereolithography (SLA) Prototyping Polymer WaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless, and look .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
BP Amoco Innovene 1088 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: ExtrusionFeatures: General purposeTypical applications: Water quenched blown filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below fr.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
Ineos H13G-00 Polypropylene Homopolymer
(discontinued **) Formerly Amoco® 7444. Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Rigid packaging, Medical componentsComplies with FDA specification, Title 21, C.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
BP Amoco Amoco® 7556 Polypropylene Homopolymer, Fiber Grade
(discontinued **) Suggested fabrication methods: Fiber spinningFeatures: High speed spinning, Improved bulk, Low gas fadeTypical applications: Upholstery, BCF carpet yarnsComplies with FDA specification, Title 21, CF.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
Ineos H00M-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; ThermoformingFeatures: High melt strength, High stiffness, Medium-term heat agingComplies with FDA specification, Title 21, CFR 177.1520.Typical application.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
BP Amoco Amoco® 7942 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Excellent mold release, AntistaticTypical applications: Closures, Thin-walled rigid packagingComplies with FDA specification, Title 21, CFR .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H38G-01 Polypropylene Homopolymer, Fiber Grade
(discontinued **) Suggested fabrication methods: Fiber spinningFeatures: Very high speed spinning, Low gas fadeTypical applications: Spunbound fabricsComplies with FDA specification, Title 21, CFR 177.1520.Typical pr.. |
|||
Izod Impact, Notched | 0.250 - 0.300 J/cm @Temperature -40.0 - -20.0 °C |
0.468 - 0.562 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.275 J/cm Grade Count:1 |
Overview of materials for Nylon 66, 40% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Mineral Filled". Specific grades with primary filler content between 35% and 44% are inclu.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H05M-00 Polypropylene Homopolymer Grade H05M-00 is a general purpose polypropylene homopolymer for injection molding applications. This resin provides good long-term heat stability. This material meets the requirements of the Food.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H13M-00 Polypropylene Homopolymer Grade H13M-00 is a general purpose polypropylene homopolymer for injection molding applications. It provides good long-term heat stability.Suggested fabrication methods: Injection moldingFeatures: .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H20H-00 Polypropylene Homopolymer This resin is designed to provide easy moldability for applications requiring resistance to long term heating. This material has been recognized by UL for sustained use at 130c.Suggested fabricatio.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | UV Postcure; ASTM D256A |
DSM Somos® BioClear Parts created with Somos® BioClear are designed for medical applications that are non-implant and have limited contact with the body such as device prototyping. They are shatter-resistant so they w.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256A |
DSM Somos® WaterShed® XC 11122 Water-resistant resin for stereolithography DescriptionWaterShed XC is a low viscosity liquid photopolymer that produces strong, tough, water-resistant, ABS-like parts. Most importantly parts created with WaterShed 11122 are nearly colorless.. |
|||
Izod Impact, Notched | 0.220 - 0.300 J/cm | 0.412 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATF 197 Phenolic Molding Inorganic and glass Filler, Compression Molded Characteristics:Flame retardantSpark resistant Good electrical insulationHeat stability ( 200°C )Good mouldability Low water absorptionLow shrinkageColor-blackSoft/medium flow Applications:Switchg.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATI 172 Phenolic Molding Organic and inorganic Filler, Injection Molded Characteristics:Heat resistant ( asbestos free )Good electric insulationLow shrinkageLow water absorptionMedium mechanical strengthNot suitable for high mechanical tensionColor-blackVery soft flow .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATS 134 Phenolic Molding Inorganic, graphite Filler, Compression Molded Characteristics: Low coefficient of frictionSelf lubricating ( graphite modified )Good thermal conductivityGood glide propertiesNot suitable for electrical applicationColor- black gray Soft/medium f.. |
|||
Izod Impact, Notched | 0.220 - 0.300 J/cm | 0.412 - 0.562 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATR 126 Phenolic Molding Organic Filler, Compression Molded Characteristics:Ammonia freeGood mouldabilityGood mechanical strengthGood electrical insulationGood surface finishMedium thermal stability Color-black, brownSoft/medium flow Applications:Telecommuni.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H14A-00 Polypropylene Homopolymer Suggested fabrication methods: Injection molding and extrusion applications.Features: AntistaticTypical applications: Packaging, Closures, Consumer productsComplies with FDA specification, Title 21,.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Temperature -40.0 - -20.0 °C |
0.375 - 0.562 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.267 J/cm Grade Count:2 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H35Z-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm | 0.375 - 0.562 ft-lb/in | ASTM D256-06 |
Proto3000 Objet VeroWhitePlus FullCure835 Rigid Opaque Prototyping Polymer Information provided by Proto3000 for their protoyping engineering services. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H07D-00 Polypropylene Homopolymer Grade H07D-00 is a polypropylene homopolymer for cast film applications that require slip and antiblock additives. This resin meets the requirements of the Food and Drug Administration as specified .. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar |
Ineos H13Z-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical prope.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
BP Amoco Amoco® Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection molding; Rotary CompressionFeatures: Nucleated, Antistatic, LubricatedTypical applications: Closures, CapsComplies with FDA specification, Title 21, CFR 177... |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H28U-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Radiation stableTypical applications: MedicalComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from inject.. |
|||
Izod Impact, Notched | 0.200 - 0.300 J/cm @Diameter 3.17 mm |
0.375 - 0.562 ft-lb/in @Diameter 0.125 in |
bar; ASTM D256 |
Ineos H35G-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Rigid packaging, Consumer products, CompoundingComplies with FDA specification, Title 21, CFR 177.1520... |