Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 2.08 J/cm | 3.90 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL SE1X PPE+PS (Asia Pacific) PPO+PS. Improved productivity and reliability. Nonchlorinated, nonbrominated flame retardant. 244F HDT. |
|||
Izod Impact, Notched | 2.08 J/cm @Thickness 3.17 mm |
3.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6 GF15 IM1 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impac.. |
|||
Izod Impact, Notched | 2.08 J/cm @Thickness 3.17 mm |
3.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill FR® ABS FR UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.08 J/cm @Thickness 3.17 mm |
3.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF55 HS L OR016 57% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 57% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File Nu.. |
|||
Izod Impact, Notched | 2.08 J/cm @Thickness 3.17 mm |
3.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF60 HS L BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Izod Impact, Notched | 2.08 J/cm @Thickness 3.17 mm |
3.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF60 X 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Izod Impact, Notched | 2.08 J/cm | 3.90 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON MV008S PP LNP VERTON* MV008S is a compound based on Polypropylene resin containing 40% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, Structural. |
|||
Izod Impact, Notched | 2.08 J/cm | 3.90 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON MV008S PP (Asia Pacific) LNP VERTON* MV008S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Izod Impact, Notched | 2.08 J/cm | 3.90 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON MV008SU PP LNP VERTON* MV008SU is a compound based on Polypropylene resin containing 40% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur.. |
|||
Izod Impact, Notched | 2.08 J/cm | 3.90 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON MV008SU PP (Asia Pacific) LNP VERTON* MV008SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Izod Impact, Notched | 2.08 J/cm | 3.90 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON MV008SU PP (Europe-Africa-Middle East) LNP VERTON* MV008SU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled, Heat Stabilized, UV-Stabilized. |
|||
Izod Impact, Notched | 2.08 J/cm | 3.90 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON MV00AS PP (Asia Pacific) LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Izod Impact, Notched | 2.08 J/cm @Temperature 23.0 °C |
3.90 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Verton MX03017 PP (Europe-Africa-Middle East) LNP* VERTON* MX03017 is a compound based on Polypropylene resin containing Glass Fiber, Long Glass Fiber. Added features of this material include: Chemically Coupled.This data was supplied by SABIC.. |
|||
Izod Impact, Notched | 2.08 J/cm | 3.90 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PN275 PPE+PS PPE+PS with low mineral loading. High heat, platable applications. |
|||
Izod Impact, Notched | 2.08 J/cm | 3.90 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL PN275F PPE+PS PPE+PS with low mineral loading. High heat, platable applications. NSF approved for water contact applications. |
|||
Izod Impact, Notched | 2.08 J/cm @Thickness 3.17 mm |
3.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF60 HS L 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Izod Impact, Notched | 2.08 J/cm @Thickness 3.17 mm |
3.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF60 TL10 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackTPCI# 8575101Information provi.. |
|||
Izod Impact, Notched | 2.08 J/cm @Thickness 3.17 mm |
3.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF70 HS L BK 70% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 70% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Izod Impact, Notched | 2.08 J/cm @Thickness 3.17 mm |
3.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PP CO GF43 CC 43% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 43% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 2.08 J/cm | 3.90 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON MV00ASXP PP (Europe-Africa-Middle East) LNP VERTON* MV00AS is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Izod Impact, Notched | 2.08 J/cm | 3.90 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL 731S PPE+PS (Asia Pacific) High heat PPO/HIPS alloy suitable for use in some potable water applications. |
|||
Izod Impact, Notched | 2.08 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
3.90 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
bar; ASTM D256 |
Diamond Polymers ASA S510 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium ImpactInformation provided by Diamond Polymers, Inc. |
|||
Izod Impact, Notched | 2.08 J/cm | 3.90 ft-lb/in | injection molded; ASTM D256 |
Americas Styrenics STYRON A-TECH® 1115 High Impact Polystyrene Product CharacteristicsHigh Gloss/High ImpactConsistent colorabilityEasy processingFood Contact CompliantTypical ApplicationsCustom high Gloss Extruded SheetRefrigeration accessoriesSmall Appliances.. |
|||
Izod Impact, Notched | 2.08 J/cm | 3.90 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON MV008SXP PP (Europe-Africa-Middle East) LNP* Verton* MV008SXP is a compound based on Polypropylene resin containing Long Glass. Added features include: Chemically Coupled, Heat Stabilized. |
|||
Izod Impact, Notched | 2.08 J/cm | 3.90 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOTUF IX02582 PA 6/12 (Asia Pacific) LNP* Thermotuf* IX02582 is a compound based on Nylon 6/12 resin containing Proprietary Filler(s). Added features of this material include: High Impact. |
|||
Izod Impact, Notched | 2.08 J/cm | 3.90 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON MV00ASU PP LNP VERTON* MV00ASU is a compound based on Polypropylene resin containing 50% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur.. |
|||
Izod Impact, Notched | 2.08 J/cm | 3.90 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP VERTON MV00ASU PP (Europe-Africa-Middle East) LNP VERTON* MV00ASU is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |