Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
Nylene® 452 Nylon 6 Dry as molded. Injection molding grade. Nylene 452 is a plasticized, injection molding nylon for use in applications requiring high flexibility, and excellent toughness and abrasion resistance. Bec.. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
Nylene® 603 Nylon 6, Extrusion Grade Dry as molded. Extrusion grade. Nylene 603 is a plasticized, high residual monomer resin designed for extrusion applications requiring excellent flexibility, high strength and good abrasion resist.. |
|||
Izod Impact, Notched | 1.90 J/cm @Thickness 3.17 mm |
3.56 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Ineos ABS Lustran® 456 Extrusion, Matte-Gloss
(discontinued **) Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Izod Impact, Notched | >= 1.90 J/cm @Temperature 23.0 °C |
>= 3.56 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
NIZHNEKAMSKNEFTEKHIM PE 4252J (524F2) High Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD4472 PC Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili.. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® HFD4472 PC (Europe-Africa-Middle East) Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili.. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
IDI Composites M-102 Thermoset Polyester, Molding Mechanical grade materials in a range of strengths with excellent moldability and molded part appearance.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 1.90 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
3.56 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUMID HI5063A(W) PA6/ABS+MF6%, High Impact Feature: Injection Molding, PA6/ABS+MF6%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
Ineos B50-35H-011 HDPE Ineos B50-35H-011 is a high density polyethylene copolymer developed for blow molding applications. It is recommended for use in applications which require a combination of high top load strength a.. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
Ineos B50-35H-176 HDPE B50-35H is a high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which require a combination of high top load strength and good environmental s.. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
Ineos B54-25H-127 HDPE B54-25H-127 is a high density polyethylene copolymer developed for blow molding. It is recommended for use in applications which require a combination of high top load strength and good environmenta.. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem GF 4950 HS HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | edgewise; ASTM D256 |
Haysite 14100 Polyester BMC, 15% Glass Reinforced The 14100 series bulk molding compound is an electrical grade material that can be compression, transfer, or injection molded. Offering good mechanical strength and excellent electrical properties, .. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
Kostat BK-STAT P048BK PP Compound BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanline.. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | Natural & Black Colors; ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP DX06313 PC (Asia Pacific) Polycarbonate base, 30% glass fiber reinforced, impact modified material. Thinwall housing, mobile phone. Some light color grades may have lower impact data than nature and black grade. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL N300X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL N300X PPE+PS (Asia Pacific) PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3708U UV Stable Copolymer Polypropylene DescriptionPolyfort® FPP 3708U is a 20% CAC03 filled UV stable copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 1227U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1227U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 1227U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1227U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.90 J/cm @Temperature 23.0 °C |
3.56 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PA341G9 Nylon 6.6, 45% Glass Fiber 45% glass fiber reinforced, high stiffness and extreme cold environment, UV stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.90 J/cm @Temperature 23.0 °C |
3.56 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek RA846 Nylon 6.6, Impact Modified Impact modified and heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 1227U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1227U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 3708U UV Stable Copolymer Polypropylene DescriptionPolyfort® FPP 3708U is a 20% CAC03 filled UV stable copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FXP 1227U UV Stable Copolymer Polypropylene DescriptionPolyfort® FXP 1227U is a 20% CAC03 filled UV stable copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
UBE UBESTA® 3030JNU Short Cycle Time Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
Buckeye Polymers BP ABS 8336 P ABS PlatingABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of processing a.. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
Adell BI-10 Nylon 6, Impact Modified Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
Adell BI-30 Nylon 6, Impact Modified Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 1.90 J/cm | 3.56 ft-lb/in | ASTM D256 |
Buckeye Polymers BP ABS 7336 ABS High Gloss & FlowABS is a copolymer of acrylonitrile and styrene, modified with butadiene rubber. ABS is primarily used for their combination of toughness, rigidity, chemical resistance, ease of pr.. |