Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 7.79 J/cm | 14.6 ft-lb/in | ASTM D256 Type A |
Quadrant EPP Symalit® PFA Tetrafluoroethylene-perfluoroalkylvinylether (ASTM Product Data Sheet) |
|||
Izod Impact, Notched | 7.80 J/cm | 14.6 ft-lb/in | Notched/Unnotched not specified; ASTM D256 |
NOVA Chemicals Novapol® HB-W355-A HDPE Blow Molding Resin Molded Plaque Properties.Applications: drums, large industrial parts.Data provided by the manufacturer. |
|||
Izod Impact, Notched | 7.79 J/cm @Temperature 23.0 °C |
14.6 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Lexan® FXD171R PC Transparent/transluscent PC for light diffusion special effects. MFR of 25.0.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 7.79 J/cm | 14.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® FXD171R PC (Asia Pacific) Transparent/transluscent PC for light diffusion special effects. MFR of 25.0. |
|||
Izod Impact, Notched | 7.80 J/cm | 14.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® SLX2231T PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Izod Impact, Notched | 7.80 J/cm | 14.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors |
|||
Izod Impact, Notched | 7.80 J/cm | 14.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® SLX2271T PC Copolymer Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Izod Impact, Notched | 7.80 J/cm | 14.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® SLX2271T PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Izod Impact, Notched | 7.81 J/cm | 14.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP COLORCOMP DX06407H PC LNP* COLORCOMP* DX06407H is an unfilled Polycarbonate. Added features of this material include: Easy Molding, Mold Release, Healthcare |
|||
Izod Impact, Notched | 7.80 J/cm @Temperature 23.0 °C |
14.6 ft-lb/in @Temperature 73.4 °F |
V-Notched 1/8"; ASTM D256 |
Kotec Carbotex K-30 Polycarbonate, General Purpose Features: Standard, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures, Safety products, E & E parts, Household applications, Le.. |
|||
Izod Impact, Notched | 7.80 J/cm @Temperature 23.0 °C |
14.6 ft-lb/in @Temperature 73.4 °F |
V-Notched 1/8"; ASTM D256 |
Kotec Carbotex K-30FR Polycarbonate, Flame Retardant Features: Non-brominated & non-chlorined flame retardant, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, E & E parts, Safety products, Househo.. |
|||
Izod Impact, Notched | 7.80 J/cm @Temperature 23.0 °C |
14.6 ft-lb/in @Temperature 73.4 °F |
V-Notched 1/8"; ASTM D256 |
Kotec Carbotex K-30MRA Polycarbonate, General Purpose, Mold Release Grade Features: Mold release, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures, Safety products, E & E parts, Household applications.. |
|||
Izod Impact, Notched | 7.80 J/cm @Temperature 23.0 °C |
14.6 ft-lb/in @Temperature 73.4 °F |
V-Notched 1/8"; ASTM D256 |
Kotec Carbotex K-30UV Polycarbonate, General Purpose, UV Stability Grade Features: UV stability, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures, Safety products, E & E parts, Household applications.. |
|||
Izod Impact, Notched | 7.80 J/cm @Temperature 23.0 °C |
14.6 ft-lb/in @Temperature 73.4 °F |
V-Notched 1/8"; ASTM D256 |
Kotec Carbotex K-30UVR Polycarbonate, General Purpose, UV Stability + Mold Release Grade Features: UV stability, Mold release, Medium viscosityApplications: OA equipment, Communications, Precision parts, Machineries, Lighting fixtures/covers, Safety products, E & E parts, Household appl.. |
|||
Izod Impact, Notched | 7.80 J/cm @Temperature 23.0 °C |
14.6 ft-lb/in @Temperature 73.4 °F |
V-Notched 1/8"; ASTM D256 |
Kotec Carbotex KFR-30 Polycarbonate, Flame Retardant Features: Non-brominated & non-chlorined flame retardant, Medium viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, E & E parts, Safety products, Househo.. |
|||
Izod Impact, Notched | 7.80 J/cm @Temperature 23.0 °C |
14.6 ft-lb/in @Temperature 73.4 °F |
V-Notched 1/8"; ASTM D256 |
Kotec Carbotex KV-30FD Polycarbonate, Food Grade Features: Food contact, Medium viscosity, Mold release, TransparentApplications: Household appliance, Kitchenware, Food packaging/containersInformation provided by Kotec Corporation |
|||
Izod Impact, Notched | 7.80 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
14.6 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa CPA-6 Toughened PA6 Features:High impactLow tendency to wrapApplications:Injection moldingSport applianceAutomobile partsPower toolsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Izod Impact, Notched | 7.79 J/cm | 14.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY D2000I PC LNP* LUBRILOY* D2000I is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, High Impact. |
|||
Izod Impact, Notched | 7.79 J/cm | 14.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRILOY D2000I PC (Asia Pacific) LNP* Lubriloy* D2000I is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched | 7.79 J/cm | 14.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-LOY Cycoloy_CA6200 PC+ABS PRELIMINARY DATA. LNP* Stat-loy* Cycoloy_CA6200 compound is a Non-ECO flame retardant, anti-static PC+ABS for ESD management. |
|||
Izod Impact, Notched | 7.80 J/cm | 14.6 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP D7001IXH PC LNP* THERMOCOMP* D7001IXH is a compound based on Polycarbonate siloxane copolymer resin containing proprietary antimicrobial additives. Designed for touch surfaces in patient critical healthcare ap.. |