Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 13.1 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
ASTM D256
Ovation Polymers Opnyl OP66UT108 Nylon 66
Ultra Tough - High Impact, Excellent retention of mechanical properties, High service temperature. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All..
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
ASTM D256
Premix Premi-Glas® 1200-25 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st..
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
ASTM D256
Premix Premi-Glas® 1200H-25 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200H-25 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go..
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS
Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che..
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® ML7693 PC Copolymer (Asia Pacific)
Medium-flow impact-modified high-flow-ductile PC copolymer. Available in black color only.
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® PC1800R PC (Europe-Africa-Middle East)
PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® SLX2432T PC Copolymer (Asia Pacific)
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors.
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
ASTM D256
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS (Asia Pacific)
Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che..
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer
Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors.
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® EXL9330S PC Copolymer (Asia Pacific)
Opaque PC-Siloxane copolymer with excellent processability. UV stabilized. UL rated V-0/5VA/CTI-PLC-2. Available in limited colors.
Izod Impact, Notched 6.99 J/cm

@Temperature 0.000 °C
13.1 ft-lb/in

@Temperature 32.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Europe-Africa-Middle East)
40 MFR LEXAN High Flow Ductile Copolymer
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® SLD3000 PC (Asia Pacific)
Antistatic colorable/opaque FR PC grade
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
ASTM D256
Solvay Specialty Polymers Ixef® 1521 Polyarylamide (PARA)  (Unverified Data**)
Ixef 1521 is a 50% glass-fiber reinforced, flame retardant polyarylamide which exhibits high strength and stiffness, outstanding surface gloss, and excellent creep resistance. - Natural: Ixef 1521/0..
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
ASTM D256
SABIC Innovative Plastics Lexan® SLX2432T PC Copolymer
Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors.
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
Reverse notched; ASTM D256
LG Chemical LUCEL N127-02 General Purpose POM, Unreinforced, Externally Lubricated, High Flow
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
Reverse notched; ASTM D256
LG Chemical LUCEL N127-AS Antistatic POM, Unreinforced, High Flow
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
Reverse notched; ASTM D256
LG Chemical LUCEL N127-WR Weather Resistant POM, Unreinforced, High Flow
LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m..
Izod Impact, Notched 7.00 J/cm

@Temperature 23.0 °C
13.1 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Lavergne VYTEEN PC 135 General Purpose Medium Viscosity Polycarbonate
Vyteen PC 135, Black, medium viscosity polycarbonate, has an excellent balance of stiffness and impact resistanceFeatures: - High heat resistance - Good processabilityInformation provided by Biegl..
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
ASTM D256A
LyondellBasell Hifaxâ„¢ ETA-5081 Thermoplastic Olefin Resin
Key Features: fractional melt flow, medium modulus, blow molding grade thermoplastic olefin resin, flexible, good impact resistance, good processabilityApplications: automotive ductwork, convoluted ..
Izod Impact, Notched 7.00 J/cm

@Temperature 23.0 °C
13.1 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics PC1800 PC (Europe-Africa-Middle East)
PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold ..
Izod Impact, Notched 7.00 J/cm

@Temperature 23.0 °C
13.1 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics PC1800R PC
PC1800R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was suppli..
Izod Impact, Notched 7.00 J/cm

@Temperature 23.0 °C
13.1 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
SABIC Innovative Plastics PC1803R PC
PC1803R resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was..
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
ASTM D256
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Europe-Africa-Middle East)
Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability.
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
ASTM D256
Styrolution Luran® S KR 2864 C Colored ASA+PC
Description: Easy flowing injection molding grade with heat resistance for parts with thin walls and/or with adverse flowpath/wall thickness ratios.Applications: Mobile phone housings.Information pr..
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
ASTM D256
SABIC Innovative Plastics PC1800 PC (Asia Pacific)
PC1800 resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold rel..
Izod Impact, Notched 7.00 J/cm

@Temperature 23.0 °C
13.1 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Polyram RamTough PZ741 Polycarbonate, UV Stabilized
UV stabilized low viscosity polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 7.00 J/cm - NB

@Temperature 23.0 °C
13.1 ft-lb/in - NB

@Temperature 73.4 °F
ASTM-D256
Polyram RamTough RZ224 Polycarbonate, Injection Molding
Polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
Izod Impact, Notched 6.99 J/cm

@Temperature 0.000 °C
13.1 ft-lb/in

@Temperature 32.0 °F
ASTM D256
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer
40 MFR LEXAN High Flow Ductile Copolymer
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
ASTM D256
SABIC Innovative Plastics PC1800R PC (Europe-Africa-Middle East)
PC1800R resin is a medium-high flow (MFR = 18 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
Izod Impact, Notched 7.00 J/cm
13.1 ft-lb/in
ASTM D256
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Europe-Africa-Middle East)
Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts..