Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.800 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Gravi-Tech™ GRV-NY-112-W-NAT Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.800 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.50 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne LubriOne™ NY-10GF/10T BLACK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.800 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Stat-Tech™ NN-30CF/000 Black Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.50 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Lubri-Tech™ PS-30GF/15T Polybutylene Terephthalate (PBT), Glass Filled, PTFE Lubricated
(discontinued Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.50 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Lubri-Tech™ ATH-000/5M Acetal-Homopolymer
(discontinued **) Description/Features:Molybdenum Disulfide LubricatedInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 3.17 mm |
1.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Lucent Polymers CPP-0307 Polypropylene, Mineral Filled, Impact Modified Recycled ContentAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 2210EPR PEI (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 830 PBT 30% GR PBTP, excellent surface finish. Typical applications are hot air gun housing assemblies, industrial glue guns, appliance housings and handles. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature -30.0 °C |
1.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® SHF4340 PBT (Europe-Africa-Middle East) 20% GF Super High Flow PBT |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 3.17 mm |
1.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® PA6/6,6 L N Nylon 6/66 Availability: North AmericaForms: PelletsAdditive: Nucleating Agent and LubricantFeatures: Copolymer, Fast Molding Cycle, Nucleated and LubricatedProcessing Method: Injection MoldingInformation prov.. |
|||
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
Total PPC 4944WZ Polypropylene, Impact Copolymer ATOFINA 4944 polypropylene is a nucleated and controlled rheology impact copolymer. 4944WZ is characterized by improved stiffness and impact resistance, as well as low shrinkage and low warpage. I.. |
|||
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
A. Schulman LUBRILON® 432 30% Glass Fiber Reinforced, PTFE Lubricated PBT Alloy Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.801 J/cm | 1.50 ft-lb/in | ASTM D256 |
Ecomass® 1080CO94 Copper Powder Filled Polyamide Alloy, Injection Molding Moderate Specific Gravity, Copper Powder Filled Polyamide (PA) Alloy, Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting and balancing.. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
Covestro Bayflex® 190 Polyurethane Elastomeric RIM, 20% Mineral Filled, MDI-based 2-Component Liquid System 0.150 in. thickness. Calcium Silicate filled. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was se.. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
E-Polymers Tekaster® F615GFR , Flame Retardant, 30% Glass Reinforced PET 30% Glass Fiber Reinforced, Flame RetardantInformation provided by E-Polymers Co. Ltd. |
|||
Izod Impact, Notched | 0.800 J/cm @Thickness 3.17 mm |
1.50 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® 8232G HS FR BK-102 25% Glass Filled PA6 (Dry) Ultramid 8232G HS FR BK-102 is a 25% glass fiber reinforced, heat stabilized, flame retardant pigmented black PA6 injection molding compound exhibiting excellent melt stability characteristics. It .. |
|||
Izod Impact, Notched | >= 0.801 J/cm | >= 1.50 ft-lb/in | ASTM D256 |
Buckeye Polymers BP PPC 0510 BLK Polypropylene Copolymer Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resis.. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON REF42 PA 66 (Asia Pacific) LNP* Stat-kon* REF42 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Fiber. |
|||
Izod Impact, Notched | 0.801 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
1.50 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
Method A, Injection Molded; ASTM D256 |
PolyOne Edgetek® ATH-30GF/000 Acetal-Homopolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Izod Impact, Notched | >= 0.801 J/cm | >= 1.50 ft-lb/in | ASTM D256 |
Buckeye Polymers BP RPP 1509 GK BLK Polypropylene, 15% Glass Filled Product Information: 15% glass reinforced polypropyleneProduct Features:Offers improved flex modulus while maintaining a low specific gravity propertyChemically coupled for improvved physical proper.. |