Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.694 J/cm @Temperature 23.0 °C |
1.30 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products G30P100-01 30% Glass Fiber Reinforced Polypropylene, Black Applications: Fender apronsUnderhood componentsStructural componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.694 J/cm @Temperature 23.0 °C |
1.30 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Ovation Polymers Nima™ NH OPP66GF25 FR 25% Glass Filled Polyamide 66 Non-Hal red phosphorous based Flame Retardant CompoundAll properties after 48hrs conditioning at 23°C/50% RH |
|||
Izod Impact, Notched | 0.694 J/cm @Temperature 22.8 °C |
1.30 ft-lb/in @Temperature 73.0 °F |
ASTM D256 |
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | Method A; ASTM D256 |
Phillips 66 COPYLENE® CR350CL-02 Polypropylene, Random Copolymer, Clarified CR350CL-02 is a clarified, random copolymer specially designed for clear injection molding applications and is formulated with lube for excellent mold release.Potential Applications: Injection moldi.. |
|||
Izod Impact, Notched | 0.694 - 2.67 J/cm | 1.30 - 5.00 ft-lb/in | Average value: 1.16 J/cm Grade Count:9 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Izod Impact, Notched | 0.694 J/cm @Temperature 23.0 °C |
1.30 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
RheTech Products F32-01 32% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Head lamp housingBracketsUnderhood componentsElectrical housingsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
Custom Resins Vexel™ E20GF30 , 30% Glass Reinforced PET
(discontinued **) Description: Vexel™ E20GF30 is a 30% glass fiber reinforced, general purpose PET. Information provided by Custom Resins. |
|||
Izod Impact, Notched | 0.694 J/cm @Thickness 3.17 mm |
1.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® J-60/30 Polypropylene Homopolymer, 30% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Notched | 0.694 J/cm @Thickness 3.17 mm |
1.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PET GF/M35 35% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 35% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 0.694 J/cm @Thickness 3.17 mm |
1.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PA6/6 GF13 SL2 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 13% Filler by WeightAdditive: Heat Stabilizer and Silicone LubricantFeatures: Lubricated and Heat StabilizedInformation pr.. |
|||
Izod Impact, Notched | 0.694 J/cm @Thickness 3.17 mm |
1.30 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 WM40 IM HS 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact ModifiedProcessin.. |
|||
Izod Impact, Notched | 0.694 J/cm @Temperature -17.8 °C |
1.30 ft-lb/in @Temperature 0.000 °F |
0.125 in (3.2 mm) sample; ASTM D256 |
Chevron Phillips EA6740 Rubber Modified Polystyrene DescriptionChevron EA6740 is a high impact polystyrene material developed for packaging applications. Its processing characteristics make EA6740 excellent for extrusion and deep-draw thermoforming... |
|||
Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
Ecomass® 1850ZD88 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting and balancing applicationsHigh Specific GravityTungsten Powder Filled Polyamide (PA6)Information provided by Technical Polymers |
|||
Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | 73°F; ASTM D256 |
Entec Hylox® 9020 PBT, 20% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
Aclo Accutech ABS ABS831G30L Glass Reinforced |
|||
Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256A |
Braskem TI4450M Impact Copolymer Polypropylene Description: Very High Flexural ModulusApplications: Suggested Uses Include Compounding, Automotive Interior Trim, Intricately Designed Parts, Thin-Walled Parts.Process: Compounding.This resin meets.. |
|||
Izod Impact, Notched | 0.694 J/cm @Thickness 3.17 mm |
1.30 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultraform N 2320 U03 UNC Q600 POM Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade. |
|||
Izod Impact, Notched | 0.694 J/cm | 1.30 ft-lb/in | ASTM D256 |
Aaron Industries AAROPRENE® CFIPP 2020 High Impact Calcium Carbonate Filled Polypropylene AAROPRENE® CFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified. |
|||
Izod Impact, Notched | 0.694 - 1.15 J/cm | 1.30 - 2.15 ft-lb/in | Average value: 0.943 J/cm Grade Count:16 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |