Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.561 J/cm @Temperature 23.0 °C |
1.05 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Ovation Polymers Nemcon™ E-PC CB Polycarbonate Nemcon E-series products are designed for use in ESDA electronic assembly environments. Nemcon E-PC CB is a carbon black-filled polycarbonate characterized by consistent moldability, recyclability,.. |
|||
Izod Impact, Notched | 0.560 J/cm @Temperature -30.0 °C |
1.05 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics GELOY FXW710SK ASA General purpose injection molding ASA with Visual Fx sparkle effect. |
|||
Izod Impact, Notched | 0.560 J/cm @Thickness 3.17 mm |
1.05 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Performance Polymers IPS II PPL-C4219 PEKK (Polyetherketoneketone) Linear Wear Grade Black pellets; Carbon fiber/PTFE/Graphite compoundInformation provided by Infinite Polymer System II. |
|||
Izod Impact, Notched | 0.560 J/cm @Thickness 3.17 mm |
1.05 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Performance Polymers IPS II PPL-C4250 PEKK (Polyetherketoneketone) Linear 30% Carbon Fiber Reinforced Molding Grade Black pelletsInformation provided by Infinite Polymer System II. |
|||
Izod Impact, Notched | 0.560 J/cm | 1.05 ft-lb/in | ASTM D256 |
SABIC PP 6711K Polypropylene Copolymer for Injection Molding Product Description: PP 6711K is a controlled rheology grade with narrow molecular weight distribution intended specifically for producing injection molded articles with high clarity, good flow pro.. |
|||
Izod Impact, Notched | 0.560 J/cm | 1.05 ft-lb/in | ASTM D256A |
LyondellBasell Pro-fax SA861 Polypropylene Random Copolymer, Cast Film Extrusion Key Features: polypropylene random copolymer resin formulated for cast film extrusion, good optical properties, excellent slip properties, FDA acceptable, improved cold temperature impact resistance.. |
|||
Izod Impact, Notched | 0.560 J/cm | 1.05 ft-lb/in | ASTM D256 |
Kolon KOCETAL® VT702 Anti-Static Grade Acetal Resin Improved antistatic effects. Applications: Products for avoiding electric contamination. Information provided by API-Kolon. |
|||
Izod Impact, Notched | 0.560 J/cm | 1.05 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP EX10404H PEI LNP* LUBRICOMP* EX10404H is a compound based on Polyetherimide containing proprietary fillers. Added features of this grade include: Wear Resistant, Healthcare. |
|||
Izod Impact, Notched | 0.560 J/cm @Temperature 23.0 °C |
1.05 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Lubricomp JL003 PES LNP* Lubricomp* JL003 is a compound based on Polyethersulfone resin containing PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.560 J/cm @Temperature 23.0 °C |
1.05 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 1110R PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 0.560 J/cm @Temperature 23.0 °C |
1.05 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 1110R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.560 J/cm @Temperature 23.0 °C |
1.05 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem 1110R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched | 0.560 J/cm | 1.05 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM HU1110 PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Izod Impact, Notched | 0.560 J/cm | 1.05 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM HU1110 PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Izod Impact, Notched | 0.560 J/cm @Temperature -30.0 °C |
1.05 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance. |
|||
Izod Impact, Notched | 0.560 J/cm @Temperature -30.0 °C |
1.05 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER (Asia Pacific) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance. |
|||
Izod Impact, Notched | 0.560 J/cm @Temperature -30.0 °C |
1.05 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics XYLEX X7300CL PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER unreinforced alloy developed for optical or lense market. Chemical resistance. |
|||
Izod Impact, Notched | 0.560 J/cm | 1.05 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON EX07311P PEI (Asia Pacific) LNP Stat-kon* EX07311P is an easy flowing ESD-safe compound based on Polyetherimide resin. This compound is developed for good dimensional stability for use in ESD Tray for Backend Semicon and HDD t.. |
|||
Izod Impact, Notched | 0.560 J/cm @Temperature 23.0 °C |
1.05 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp XF006S LNP* Thermocomp* XF006S is a compound based on Amorphous Nylon containing Glass Fiber. Characteristics of this grade are: Heat Stabilized.This data was supplied by SABIC-IP for the Americas region.. |
|||
Izod Impact, Notched | 0.560 J/cm | 1.05 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP XF006S PA LNP* THERMOCOMP* XF006S is a compound based on Amorphous Nylon containing 30% Glass Fiber. Added feature of th is grade is: Heat Stabilized. |
|||
Izod Impact, Notched | 0.560 J/cm @Temperature 23.0 °C |
1.05 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem H 604 Blow Molding Polypropylene Applications: Transparent bottles for mineral water, cosmetic, health care and cleaning products. Information provided by Braskem |
|||
Izod Impact, Notched | 0.560 J/cm | 1.05 ft-lb/in | ASTM D256 |
Plenco 1581 Polyester, Briquette, Transfer Molded PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f.. |
|||
Izod Impact, Notched | 0.560 J/cm | 1.05 ft-lb/in | ASTM D256 |
Plenco 50335 PET, Pellet, Injection Molded, White
(discontinued **) PLENCO 50335 is an engineering grade glass reinforced polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in white, natural, and black.Inform.. |