Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.380 J/cm @Temperature -30.0 °C |
0.712 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® C7240P PC+ABS (Asia Pacific) Cycoloy* C7240P resin is a mineral filled, flame retardant PC/ABS. High stiffness combined with balanced flow and impact performance, makes it a good condidate for various applications. |
|||
Izod Impact, Notched | 0.380 - 6.40 J/cm @Temperature -50.0 - 0.000 °C |
0.712 - 12.0 ft-lb/in @Temperature -58.0 - 32.0 °F |
Average value: 2.90 J/cm Grade Count:224 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
Ineos J60-1700-173 HDPE J60-1700-173 is a high density polyethylene homopolymer. This resin is a product of Ineos' technology and is characterized by a narrow molecular weight distribution. Parts fabricated from this mater.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature 23.0 °C |
0.712 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
IRPC Polimaxx Polene 3342R Polypropylene Random Copolymer CHARACTERISTICS: HIGH CLARITY, HIGH FLOW, GOOD PROCESSABILITY APPLICATIONS: INJECTION MOLDING FOR FOOD CONTAINERS, HOUSEWARES, CRATES |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -20.0 °C |
0.712 ft-lb/in @Temperature -4.00 °F |
|
Kuraray HYBRAR® PH4 Polypropylene Blend Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Izod Impact, Notched | >= 0.380 J/cm | >= 0.712 ft-lb/in | Method A; ASTM D 256 |
Karina 805-10/152-A-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP ML003S PP LNP* LUBRICOMP* ML003S is a compound based on Polypropylene resin containing 15% PTFE. Added features include: Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -30.0 °C |
0.712 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM EXUM0167 PEI Blend Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 325FC PBT (Europe-Africa-Middle East) Commercial, VALOX 325FC is compliant with food contact regulations. VALOX 325FC is a general purpose, unreinforced PBT injection moulding resin which contains internal mold release. This new 325FC g.. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON OEL32 PPS - Linear LNP* STAT-KON* OCL32 is a compound based on PPS - Linear resin containing 10% Carbon Fiber, 15% PTFE. Added features of this grade include: Electrically Conductive, Wear Resistant. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
SPS Guang Zhou SAMATâ„¢ 168(f1) Flame-retarded Polypropylene Characteristic: Good flame resistance, good chemical resistance, good mechanical propertiesApplications: X'mas decorative product, E/E applianceInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP WH0200B PBT LNP* Thermocomp* WH0200B is a compound based on PBT resin containing proprietary fillers. Added features include: High Specific Gravity. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -30.0 °C |
0.712 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -30.0 °C |
0.712 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Asia Pacific) Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP QFL32 PA 6/10 LNP* LUBRICOMP* QFL32 is a compound based on Nylon 6/10 containing 10% Glass Fiber, 15% PTFE. Added features of this grade include: Wear Resistant. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -30.0 °C |
0.712 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM AUT210 PEI Transparent, Thermoplastic Polyimide (TPI). Glass transition Temperature (Tg) of 227degC. Haze onset temperature of 212degC (SABIC IP method). Very low outgassing and plateout, for automotive lighti.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -30.0 °C |
0.712 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM AUT210 PEI (Asia Pacific) Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -30.0 °C |
0.712 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics ULTEM AUT210 PEI (Europe-Africa-Middle East) Transparent Polyetherimide (Tg 227 degC). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature o.. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MF002S PP LNP* Thermocomp* MF002S is a compound based on Polypropylene resin containing 10% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature -30.0 °C |
0.712 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL LTA1350 PPE+PS (Europe-Africa-Middle East) Noryl* LTA1350 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
Plenco 1581 Polyester, Pellet, Injection Molded PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f.. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
Toyobo VYLOPET® EMC317A Injection Molding Polyester Resin, Warpageless Applications: Iron's heat insulation plateChair framesHousingsFeatures: WarpagelessInformation provided by Toyobo. |
|||
Izod Impact, Notched | 0.380 J/cm @Thickness 3.20 mm |
0.712 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Beijing Chemical Industry KAIFA® GL5100 ABS Extrusion Grade Non-toxic, Superior impact strength at low temp., High gloss, Uniform sheet thickness for vacuum moldingInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Izod Impact, Notched | 0.380 - 1.50 J/cm @Temperature -40.0 - -20.0 °C |
0.712 - 2.81 ft-lb/in @Temperature -40.0 - -4.00 °F |
Average value: 0.940 J/cm Grade Count:1 |
Overview of materials for Low Density Polyethylene (LDPE), Molded This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Molded". Each property range of values reported is minimum and maximum .. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL FP6130 PPE+PS Noryl* FP6130 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR a.. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics NORYL RN0611 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0611 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America Epiall® 1914A Short Glass Fiber Reinforced Epoxy Epiall 1914A is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided by.. |
|||
Izod Impact, Notched | 0.380 J/cm | 0.712 ft-lb/in | ASTM D256 |
Sumitomo Bakelite North America RX® 647 Fiberglass Reinforced Phenolic RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10. RX 647 is a fibe.. |
|||
Izod Impact, Notched | 0.380 J/cm @Temperature 23.0 °C |
0.712 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Braskem H 606 Thermoforming Polypropylene Description: H 606 is low melt flow rate homopolymer with general purpose additive package. This resin is designed for extrusion and thermoforming. H 606 presents excellent processability and high o.. |