Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | ASTM D256 |
NCMT NanoPAC™ S216 High Performance Polypropylene Nanocomposite Characteristics: High stiffness Supplementary of ABS Good impact resistant Less shrinkage Good thermal conductivity Applications: Toys Industry AutomobileInformation provided by Nano Composite Mater.. |
|||
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | ASTM D256 |
SABIC MG200024 Linear Low Density Polyethylene for Compounding Product Description: MG200024 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution primarily suitable for compounding. It is in the powder form designed to give g.. |
|||
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | ASTM D256 |
SABIC MG500026 Linear Low Density Polyethylene for Compounding Product Description: MG500026 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution primarily suitable for compounding applications. It is in the powder form and h.. |
|||
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2200-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2200-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2203-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2203-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2204-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 2205-15 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2205-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | ASTM D256 |
Premix Premi-Glas® 3200-15 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-15 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® C6840 PC+ABS (Asia Pacific) Cycoloy* C6840 resin is an injection moldable, flame retardant PC/ABS blend. It contains non-chlorinated & non-brominated flame retardant systems intended to meet governmental regulations and variou.. |
|||
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CE1821 PC+ABS High stiffness PC/ABS blend offering high impact, high heat, low CTE, good surface quality and excellent extrusion and thermoforming characteristics. |
|||
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Asia Pacific) Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature -30.0 °C |
9.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® IP1000 PC+ABS Automotive applications: High impact and ductility to -22F for interior trim and instrument panel applications. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature -30.0 °C |
9.37 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® IP1000 PC+ABS (Asia Pacific) IP1000 is a high impact PC/ABS blend developed for the automotive instrument panel business. |
|||
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® RCY6113 PC+ABS (Asia Pacific) Cycoloy* RCY6113 resin is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant. It contains 30% post consumer recycle content with a UL-94 5VB rating @ 2.0mm an.. |
|||
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Cycoloy® XCM830 PC+ABS PC/ABS with high stiffness and impact performance |
|||
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | ASTM D256 |
SABIC M500026 Linear Low Density Polyethylene for Injection Molding Product Description: M500026 is a Linear Low Density Polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to give excell.. |
|||
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | ASTM D256 |
Gichem GIBLEND F70500 Polycarbonate / ABS
(discontinued **) Polycarbonate and ABS blend, excellent mechanical and thermal properties, very high fluidity. Medium Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | Reverse notched; ASTM D256 |
LG Chemical LUCEL WK-320 Wear Resistant POM, 20% Mineral Filled, High Modulus LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 5.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
9.37 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa MAC-601 AC PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic partsComputer and accessoriesHou.. |
|||
Izod Impact, Notched | 5.00 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
9.37 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa MAC-701 PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic p.. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 0.000 °C |
9.37 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC (Asia Pacific) Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 23.0 °C |
9.37 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek RD101 Nylon 12, Injection Molding Outstanding flexibility polyamide 12 for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 23.0 °C |
9.37 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamLloy PBB701 PC/ABS alloy, UV Stabilized UV stabilized PC/ABS alloy for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.00 J/cm @Temperature 23.0 °C |
9.37 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram Polytron A60B02 Nylon 66, Chemically Coupled 60% Long Fiber A CHEMICALLY COUPLED 60% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTIONInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ CFP 4611 11% CACO3 filled copolymer polypropylene product DescriptionPolyfort® CFP 4611 is an 11% CACO3 filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 5.00 J/cm | 9.37 ft-lb/in | ASTM D256 |
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane Information provided by A. Schulman. |