Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.55 J/cm | 2.90 ft-lb/in | ASTM D256 Type A |
Quadrant EPP PPO Polyphenylene oxide, unfilled, extruded (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products. |
|||
Izod Impact, Notched | 1.55 - 4.27 J/cm | 2.90 - 8.00 ft-lb/in | Average value: 2.82 J/cm Grade Count:8 |
Overview of materials for Polyphenylene Ether, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, Impact Grade". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 1.55 J/cm | 2.90 ft-lb/in | 0.25 in; ASTM D256 |
Ravago Manufacturing Americas Hylac® FR134 ABS Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava.. |
|||
Izod Impact, Notched | 1.55 J/cm @Thickness 3.17 mm |
2.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® J-68/30/E Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Notched | 1.55 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.90 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PA6-MG30 30% Glass & Mineral Filled PA6 Features:Low tendency to wrapExcellent size stabilityLow abrasionOutstanding surfaceApplications:Injection moldingAutomobile partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Izod Impact, Notched | 1.55 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
2.90 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa PA66-T15 15% Mineral Filled PA66 Features:Good size stabilityLow tendency to wrapGood surfaceExcellent balance propertiesApplications:Injection moldingAutomobile partsPower toolsSport applianceInformation Provided by Kingfa Sci. & .. |
|||
Izod Impact, Notched | 1.55 J/cm @Thickness 3.17 mm |
2.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA12 GF30 HS L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformati.. |
|||
Izod Impact, Notched | 1.55 J/cm @Thickness 3.17 mm |
2.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA12 GF30 L 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.55 J/cm @Thickness 3.17 mm |
2.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6/6 GF55 HS L 55% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 55% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File Nu.. |
|||
Izod Impact, Notched | 1.55 J/cm @Thickness 3.17 mm |
2.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Statiblend® PA6 GF30 AS BK 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: AntistaticFeatures: AntistaticAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.55 J/cm @Thickness 3.17 mm |
2.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA12 GF50 L 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 1.55 J/cm | 2.90 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1605 Glass Reinforced Chemically Coupled Copolymer DescriptionPolyfort® FPP 1605 is a 10% glass reinforced chemically coupled copolymer. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.55 J/cm | 2.90 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® PC120GR Polycarbonate, 20% Glass Fiber Reinforced, Mold Release Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 1.55 J/cm | 2.90 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1605 Glass Reinforced Chemically Coupled Copolymer DescriptionPolyfort® FPP 1605 is a 10% glass reinforced chemically coupled copolymer. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.55 J/cm | 2.90 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1605 Glass Reinforced Chemically Coupled Copolymer DescriptionPolyfort® FPP 1605 is a 10% glass reinforced chemically coupled copolymer. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.55 J/cm | 2.90 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1605 Glass Reinforced Chemically Coupled Copolymer DescriptionPolyfort® FPP 1605 is a 10% glass reinforced chemically coupled copolymer. It has good impact and heat resistance. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.55 J/cm | 2.90 ft-lb/in | ASTM D256 |
Total PSI 960E Polystyrene Polystyrene 960E is a high impact polystyrene designed for extrusion/thermoforming applications that require exceptional resistance to attack from fats and oils. This ESCR material is used for lids .. |
|||
Izod Impact, Notched | 1.55 J/cm | 2.90 ft-lb/in | ASTM D256 |
Ecomass® 1080ZD92 Tungsten Powder Filled Polyamide Alloy, Injection Molding Grade High Specific Gravity, Tungsten Powder Filled Polyamide (PA) Alloy, Excellent Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing.. |
|||
Izod Impact, Notched | 1.55 J/cm @Thickness 3.17 mm |
2.90 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultraform N 2640 Z6 UNC POM Ultraform N 2640 Z6 UNC is an elastomer-modified injection molding POM grade with excellent impact strength. |
|||
Izod Impact, Notched | 1.55 J/cm @Thickness 3.17 mm |
2.90 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® 8272G HS BK-102 12% Glass Filled PA6 (Conditioned) Ultramid 8272G HS BK-102 is a 12% glass fiber reinforced, black pigmented, thermally modified, nylon 6 blow molding compound offering an excellent balance of engineering properties combined with the.. |
|||
Izod Impact, Notched | 1.55 J/cm @Temperature -40.0 °C |
2.90 ft-lb/in @Temperature -40.0 °F |
ASTM Test |
BASF Ultramid® 8350 HS PA6 (Conditioned) Ultramid 8350 HS is a heat stabilized, impact modified type 6 graft copolymer developed for extrusion, tubing, and jacketing applications requiring a high level of toughness combined with a moderate.. |
|||
Izod Impact, Notched | 1.55 J/cm | 2.90 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 527-13G Nylon 66, 13% Glass Reinforced A 13% glass reinforced, impact modified Nylon 66.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.55 J/cm | 2.90 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 527LD-14G Nylon 66, 14% Glass Reinforced A high impact nylon with 14% glass.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.55 J/cm | 2.90 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® F242 ABS Flame retardant.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.55 J/cm @Thickness 6.35 mm |
2.90 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall ProTherm® 4353 Rigid PVC, Extrusion Georgia Gulf ProTherm® 4353 is a CPVC powder blend designed for extrusion of large diameter, heavy wall industrial pipe requiring high temperature and good chemical resistance. Processing and stab.. |
|||
Izod Impact, Notched | >= 1.55 J/cm | >= 2.90 ft-lb/in | IS 13411-1992 |
Amity Thermosets ATS 766 Phenolic Molding Chopped cotton fabric Filler, Compression Molded Characteristics:High impact strengthGlossy surfaceLow shrinkageGood sliding propertiesColor-BrownMedium flowApplications:Cog wheelsCastor wheelsBush bearingsPulleysWelding rod handlesTextile bobbins.. |
|||
Izod Impact, Notched | 1.55 J/cm @Diameter 3.17 mm |
2.90 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 5420 High Impact Polystyrene
(discontinued **) High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheetProperties were determined on injection m.. |
|||
Izod Impact, Notched | 1.55 J/cm @Thickness 3.17 mm |
2.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
PlastxWorld CEVIAN® A1700 PA/ABS Alloy, DAM Property data is for dry as molded (DAM) samples.Information provided by PlastxWorld Inc. |
|||
Izod Impact, Notched | 1.55 J/cm @Thickness 3.17 mm |
2.90 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Fiberfil® J-68/30/E/UV Polypropylene Copolymer, 30% Glass Fiber Reinforced, Chemically coupled, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Izod Impact, Notched | 1.55 J/cm @Temperature 23.0 °C |
2.90 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PB312J6 Nylon 6, 30% Glass Fiber 30% glass-fiber reinforced polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |