| Category | Polymer , Thermoplastic , Polyphenylene Ether/PPO |
| Manufacturer | Quadrant Engineering Plastics Products |
| Trade Name | PPO |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Quadrant EPP PPO Polyphenylene oxide, unfilled, extruded (ASTM Product Data Sheet).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.08 g/cc | 1.08 g/cc | ASTM D792 |
| Water Absorption | 0.10 % | 0.10 % | Immersion, 24hr; ASTM D570(2) |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell M | 92 | 92 | ASTM D785 |
| Tensile Strength | 57.2 MPa | 8300 psi | ASTM D638 |
| Elongation at Break | 23 % | 23 % | ASTM D638 |
| Tensile Modulus | 2.53 GPa | 367 ksi | ASTM D638 |
| Flexural Strength | 88.9 MPa | 12900 psi | ASTM D790 |
| Flexural Modulus | 2.74 GPa | 397 ksi | ASTM D790 |
| Compressive Strength | 91.0 MPa | 13200 psi | 10% Def.; ASTM D695 |
| Compressive Modulus | 2.18 GPa | 316 ksi | ASTM D695 |
| Shear Strength | 57.2 MPa | 8300 psi | ASTM D732 |
| Izod Impact, Notched | 1.55 J/cm | 2.90 ft-lb/in | ASTM D256 Type A |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 64.1 µm/m-°C <br>@Temperature -40.0 - 149 °C |
35.6 µin/in-°F <br>@Temperature -40.0 - 300 °F |
ASTM E831 |
| Maximum Service Temperature, Air | 93.3 °C | 200 °F | Long Term |
| Deflection Temperature at 1.8 MPa (264 psi) | 127 °C | 260 °F | ASTM D648 |
| Glass Transition Temp, Tg | 140 °C | 284 °F | ASTM D3418 |
| Flammability, UL94 | V-1 | V-1 | 1/8 inch (Estimated Rating) |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistivity per Square | >= 1e+13 ohm | >= 1e+13 ohm | EOS/ESD S11.11 |
| Dielectric Strength | 27.6 kV/mm | 701 kV/in | Short Term; ASTM D149 |
| Compliance Properties | Metric | English | Comments |
|---|---|---|---|
| 3A-Dairy | No | No | |
| Canada AG | No | No | |
| FDA | No | No | |
| USDA | No | No | |
| USP Class VI | No | No |
| Chemical Resistance Properties | Metric | English | Comments |
|---|---|---|---|
| Acids, Strong (pH 1-3) | Unacceptable | Unacceptable | |
| Acids, Weak | Acceptable | Acceptable | |
| Alcohols | Acceptable | Acceptable | |
| Alkalies, Strong (pH 11-14) | Unacceptable | Unacceptable | |
| Alkalies, Weak | Acceptable | Acceptable | |
| Chlorinated Solvents | Unacceptable | Unacceptable | |
| Conductive / Static Dissipative | No | No | |
| Continuous Sunlight | Limited | Limited | |
| Hot Water / Steam | Limited | Limited | |
| Hydrocarbons - Aliphatic | Limited | Limited | |
| Hydrocarbons - Aromatic | Unacceptable | Unacceptable | |
| Inorganic Salt Solutions | Acceptable | Acceptable | |
| Ketones, Esters | Unacceptable | Unacceptable |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Black | |
| Machinability | 6 | 1-10, 1=Easier to Machine |