Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
Nylene® Norpex® AX20GF , 20% Glass Reinforced Polyphenylene Ether Description: Norpex® AX20GF us a 20% glass fiber reinforced Polyphenylene Ether. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric.. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers NPP 25-1011B Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 1.12 J/cm @Temperature -30.0 °C |
2.10 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® FST9705 PC Copolymer (Europe-Africa-Middle East) High viscosity PC Copolymer, OSU 55/55 compliant, low smoke, flame retardant resin |
|||
Izod Impact, Notched | 1.12 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
2.10 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D-256 |
Chevron Phillips EC6400 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Packaging and one-time use itemsPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Very good printabilityMatte surface .. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM Data |
Americas Styrenics Styron® 8100 MFD High Impact Polystyrene
(discontinued **) STYRON 8100 MFD high impact polystyrene is designed for microfloppy diskettes (MFD) applications. It offers easy processing, coloring, abrasion resistance, impact strength, and high heat resistance... |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | |
Resin Technology Group TIGA 101-EX Five-Minute Epoxy Adhesive 1 part resin to 1 part hardener.TIGA 101-EX is an exceptional epoxy formulation, recommended for lower temperature or wet industrial bonding applications where fast curing is required. This clear, t.. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC (Asia Pacific) 20% glass reinforced/15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM 2410 PEI 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Izod Impact, Notched | 1.12 J/cm @Thickness 3.17 mm |
2.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PA6 GF15 IM BK 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by Weight Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedAppearan.. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF008ESY PA 66 LNP THERMOCOMP* RF008ESY is a compound based on Nylon 66 resin containing 40% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Izod Impact, Notched | 1.12 J/cm @Temperature -30.0 °C |
2.10 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX9400W PPE+PS+PA (Asia Pacific) High flow PPO+PA. Power distribution box applications. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM HU2410 PEI 40% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP.. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman... |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 6 GF15H 30% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
A. Schulman SCHULAMID® 6 GF15H 30% Glass Fiber Reinforced Nylon 6 Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
Total PSI 830 Polystyrene Polystyrene 830 is a high melt flow, high impact polystyrene specially designed for hard to fill injection molding applications. The high flow 830 material aids production of stress free parts.The m.. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy® E-14756 Flame Retardant Easy Flow Polycarbonate Alloy Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
Formosa Plastics Formolene® 2510A Injection Applications Polypropylene Impact Copolymer with Nucleating, Antistat AdditivesApplications: Closures, housewares, small appliances, battery cases and lids.Formolene 2510A is a medium impact copolymer of polypropylene charact.. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
Ecomass® 1050ZB92 Filled Polyamide Nontoxic alternative to Lead (Pb), radiation shielding applications.Moderate Specific GravityFilled Polyamide (PA) alloyGood ToughnessInformation provided by Technical Polymers |
|||
Izod Impact, Notched | 1.12 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
2.10 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D-256 |
Chevron Phillips EB6400 HIPS - High Impact Polystyrene Rubber modified high impact polystyrene.Applications:Packaging and one-time use itemsPrinted toys and gamesPoint of purchase displaysSilk screen printingFeatures:Very good printabilityMatte surface .. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 525-33G Nylon 66, 33% Glass Reinforced High impact Nylon 66 reinforced with 33% glass fibers, lubricated.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
Asahi Kasei Thermylene® P7-40FG-0790 40% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 520-25GU Nylon 66, 25% Glass Reinforced Nylon 66, 25% glass reinforced resin, utility grade.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.12 J/cm @Diameter 3.17 mm |
2.10 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 5100 High Impact Polystyrene
(discontinued **) Good balance of toughness and rigidity, USP Class VIApplications: Spools and reels, Thermoformed and molded packaging, Photographic cartridges, AppliancesProperties were determined on injection mold.. |
|||
Izod Impact, Notched | 1.12 J/cm @Diameter 3.17 mm |
2.10 ft-lb/in @Diameter 0.125 in |
bar, 0.010" notch radius; ASTM D256 |
Ineos Nova 5104 High Impact Polystyrene
(discontinued **) Good balance of toughness and rigidity, USP Class VIApplications: Spools and reels, Thermoformed and molded packaging, Photographic cartridges, AppliancesProperties were determined on injection mold.. |
|||
Izod Impact, Notched | 1.12 J/cm | 2.10 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. .. |
|||
Izod Impact, Notched | 1.12 J/cm @Thickness 3.17 mm |
2.10 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® SPS GF40 BK 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightFeatures: SyndiotacticAppearance: BlackInformation provided by TP Composites, Inc. |