Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.800 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ PPR-40G Nat Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | 0.800 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ X MX5210-0030 RS Natural Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature -30.0 °C |
1.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Cycoloy® CY5100 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering excellent flow / impact balance for large size applications |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature -30.0 °C |
1.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Lexan® 505R PC (Asia Pacific) Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm... |
|||
Izod Impact, Notched | 0.800 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.50 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Geon™ Vinyl Fittings 210A White 271(HS) Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
Covestro Petlon® 4630 Semi-Crystalline PET, 30% Glass Fiber
(discontinued **) Characteristics: Flame Retardant: Electrical Properties, High Heat and Chemical ResistanceApplications: Connectors, Relays, Switches, Automotive (Under Hood), AppliancesProcessing: Injection Molding.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL GP-1000FA General Purpose Polypropylene, High Impact, Flame Retardant, Non-Bleed LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive: Bumper cover, instrument panel, glove box, air cleaner.. |
|||
Izod Impact, Notched | 0.800 - 1.00 J/cm | 1.50 - 1.87 ft-lb/in | ASTM D256 |
Loxim 820 01 HBCC Polypropylene Compound, 20% Chemically Coupled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.800 J/cm @Thickness 3.20 mm, Temperature -40.0 °C |
1.50 ft-lb/in @Thickness 0.126 in, Temperature -40.0 °F |
ASTM D256 |
Ineos ABS TRIAX® 1120 ABS/Nylon Blend, Injection Grade, As Conditioned Injection molding grade with good flow and stress corrosion cracking resistance, good chemical resistance (fuel, cleaning agents), high impact and notched impact strength, good acoustical damping be.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Izod Impact, Notched | 0.800 J/cm @Thickness 3.18 mm |
1.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® R-4-200BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-200NA and R-4-200BL 40% glass fiber reinforced polyphenylene sulfide compounds provide enhanced mechanical strength and low maintenance molding using conventional molding equipmentFeat.. |
|||
Izod Impact, Notched | 0.800 J/cm @Thickness 3.18 mm |
1.50 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Solvay Specialty Polymers Ryton® R-4-230BL Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4-230NA and R-4-230BL 40% glass fiber reinforced polyphenylene sulfide compounds provide reduced flash and improved processability compared to other polyphenylene sulfide injection moldi.. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 0.000 °C |
1.50 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East) VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature -30.0 °C |
1.50 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East) VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 830F PBT+PET PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Valox® 830R PBT (Asia Pacific) 30% glass filled, release grade, polyester alloy.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® 865 PBT+PET (Asia Pacific) 30% GR PBTP, UL94 V-0 rated. Non-blooming flame retardant. Improved surface appearance. Same application areas as for VALOX 855. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific) Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT.. |
|||
Izod Impact, Notched | 0.800 J/cm @Thickness 3.20 mm |
1.50 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Supreme Petrochem SP6489 9940 High Impact Polystyrene Characteristics High flow Good toughness Available in black only Processing Injection moldingApplications TV and audio-video back and front cover Material Status: Commercial : ActiveAgency Ratings.. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | 40 min.; ASTM D256 |
A. Schulman PP 1329 Polypropylene Stabilized Copolymer Polypropylene DescriptionPolypropylene PP 1329 is a stabilized copolymer polypropylene. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram PlusTek PB300G5 Nylon 6, 15% Glass Fiber 15% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamOfin PPH302G4 Polypropylene, 20% Glass Fiber 20% glass fiber reinforced polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1239H Glass Filled Chemically Coupled Homopolymer Polypropylene DescriptionPolyfort® FPP 1239H is a 30% glass filled chemically coupled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.800 J/cm @Temperature 23.0 °C |
1.50 ft-lb/in @Temperature 73.4 °F |
ASTM-D256 |
Polyram RamOfin PPH300J8 Polypropylene, 40% Glass Fiber 40% glass fiber and glass beads reinforced, high stiffness polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
Adell ER-34 Homopolymer Polypropylene, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Notched | 0.800 J/cm @Thickness 3.17 mm |
1.50 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® 8281 HS PA6 (Dry) |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 640 Nylon 6/12, Glass/Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
Gharda Chemicals GATONE™ 5330CF Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
Izod Impact, Notched | 0.800 J/cm | 1.50 ft-lb/in | ASTM D256 |
Solvay TECHNYL® A 218 PA66, 33% glass fiber, DRY Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addit.. |