Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | ASTM D256 |
PolyMirae Moplen EP540S Injection Molding Grade Polypropylene Moplen EP540S is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP540S is a block copolymer particularly suitable for injection.. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | DIN 53453; ASTM D256 |
Kolon SPESIN® KP213G45 Flame Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUCEL N109WR POM, Chemical Resistance Feature: Injection Molding, POM, Chemical ResistanceApplication: Automotive Air-conditioner Valve, Fuel Tank Cap, etc.CAS No. 66455-31-0Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUCON SP9306FL sPS+MF Description Injection Molding Grade, sPS+MF, Low Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts CAS No. 9003-53-6, 65997-17-3, 68928-70-1 .. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN136 General Purpose Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Izod Impact, Notched | >= 0.686 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 1.29 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL GP2200 PP+GF20% Description: Injection Molding, PP+GF20%, General PurposeApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPET® KP133G30 FR-PET Resin KOPET® is the FR-PET which realizes the good properties and surface of injection molding with good mold process of short cooling time in low molding temperature.Good mold release, good surface of.. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP5106F PC/ABS+GF10%, Flame Retardance Description: Injection Molding, PC/ABS+GF10%, Flame RetardanceApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOY GP5206F PC/ABS+GF20%, Flame Retardance Description: Injection Molding, PC/ABS+GF20%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG.. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUSEP GP2400 PPS+GF40%, General Purpose Feature: Injection Molding, PPS+GF40%, General PurposeApplication: Pump Units, Motor Units, etc.CAS No. 25212-74-2 and 65997-17-3Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.686 J/cm @Temperature 23.0 °C |
1.29 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUTENE-H ME5000 HDPE Description: LUTENE-H ME5000 is mainly intended for injection molding of containers and bottle cap. It has good stress cracking resistance and high impact strength.Applications: Containers, dust bin.. |
|||
Izod Impact, Notched | 0.686 J/cm @Temperature 23.0 °C |
1.29 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical SEETEC M1600 Polypropylene Impact Copolymer Features: SEETEC M1600 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1600 exhibits a high flowability and a good balance of stiffness and impact strength. SEE.. |
|||
Izod Impact, Notched | >= 0.686 J/cm @Thickness 6.35 mm |
>= 1.29 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax PBT 5130-104 30% Glass Fiber Filled CCP Halogen-free PBT, Black. PBT flame-retarded glass fiber 30% reinforced injection molding gradeCharacteristics:Excellent electrical property Excellent temperature resistance, high heat distortion.. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN133MT40 M/F Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN135HB40SIBL Multi Reinforced Nylon 6 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in automobile and industrial parts.Good mechanical properties, outstanding self-lubr.. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN3311N General Purpose Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | DIN 53453; ASTM D256 |
Kolon KOPA® KN331F General Purpose Nylon 66 KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.High tensile strength, outstandin.. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | |
Shinil Chemical SHINFLAME PA-66 GF Flame Retardant Polymer Under Hood SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod.. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® F202G30 PBT, 30% Glass Filled, Fire Retardant, Halogen Free Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.17 mm |
1.29 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® GR-4015A ABS, Glass Filled Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
1.29 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Shinkong Synthetic Fibers Shinite® F202G30 PBT, 30% Glass Filled, Fire Retardant, Halogen Free Information from Shinkong Synthetic Fibers Corp. |
|||
Izod Impact, Notched | 0.686 J/cm @Thickness 3.17 mm |
1.29 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® VB-5305G PBT, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | ASTM D256 |
Cheng Yu Plastic N66C3 Nylon 66, 30% Mineral Reinforced |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | ASTM D256 |
Cheng Yu Plastic T882GV15 Flame Retardant PBT, 15% Glass Fiber |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | ASTM D256 |
Cheng Yu Plastic T888G15 PBT, 15% Glass Fiber |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | ASTM D256 |
Cheng Yu Plastic FV3050 Polyformaldehyde |
|||
Izod Impact, Notched | 0.686 J/cm - NB | 1.29 ft-lb/in - NB | Average value: 2.14 J/cm Grade Count:22 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |
|||
Izod Impact, Notched | >= 0.686 J/cm @Thickness 6.35 mm |
>= 1.29 ft-lb/in @Thickness 0.250 in |
ASTM D256 |
Gromax CCP PBT 6730-104F Glass/Mineral Filled Product Description: PBT glass/mineral reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellent w.. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | DIN 53453; ASTM D256 |
Kolon SPESIN® KP213G15 Flame Retardant PBT Resin
(discontinued **) SPESIN® is a thermoplastic PBT resin with excellent thermal, mechanical and electrical properties. SPESIN® is widely used in industrial parts and especially in electrical-electronic parts.High hea.. |
|||
Izod Impact, Notched | 0.686 J/cm | 1.29 ft-lb/in | ASTM D256 |
E-Polymers TEKAFIN® PH50GM 30% Glass Fiber Reinforced Mineral Filled Low Warpage Compounded-PP Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.I.. |