Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256-93a |
Multibase Multi-Pro® 3012 RC 30% Glass Filled Polypropylene Moisture content is 0.06%. Multi-Pro 3012 RC is a glass reinforced polypropylene, chemically coupled which enhances the mechanical properties. This product has been formulated to achieve an esthe.. |
|||
Izod Impact, Notched | 0.590 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.11 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ PPC-20T Nat Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | 0.590 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.11 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ 600 A Zip 22 Natural Polyamide 6 Alloy (Nylon 6 Alloy) The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials.. |
|||
Izod Impact, Notched | 0.590 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.11 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Trilliant™ HC X HC5200-0025 RS Natural Polypropylene Copolymer (PP Copolymer) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.590 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.11 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® PF-05GF/000 FR MR Polysulfone (PSU) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
PolyOne Edgetek® PS-20GF/000 NATURAL Polybutylene Terephthalate (PBT) Information provided by PolyOne |
|||
Izod Impact, Notched | 0.590 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.11 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded, Across Flow; ASTM D256A |
PolyOne Nymax™ 1200 A L Natural Polyamide 66 (Nylon 66) The Nymax® 1200 Blend Series of nylon 6/6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materi.. |
|||
Izod Impact, Notched | 0.590 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
1.11 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ GF 1200 A 13 HS Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Izod Impact, Notched | 0.590 - 1.17 J/cm | 1.11 - 2.20 ft-lb/in | Average value: 0.950 J/cm Grade Count:5 |
Overview of materials for Polyphenylene Ether, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, PTFE Filled". Each property range of values reported is minimum and maximum values .. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Chevron Phillips HiD® 9706 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear homopolymerCharacteristics: moderate flow, good impact strength, excellent stiffness, good ESCR, moderate shrinkage resistanceApplications: crates and totes, structural foamInform.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM CRS5011R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics and ketones. Resin is RoHS compliant. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON AE008XXY ABS LNP* STAT-KON* AE008XXY is a compound based on ABS resin containing 40% Carbon Fiber. Added feature of this material ia: Electrically Conductive. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON DC10EPFR PC LNP* STAT-KON* Lexan_DC10EPFR is a compound based on Polycarbonate containing Carbon Fiber. Added features of this grade include: Exceptional Processing, Flame Retardant, Electrically Conductive. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics ULTEM UF5011S PEI (Asia Pacific) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Veradel® AG-320 Polyethersulfone (PESU), 20% Glass Fiber Veradel® AG-320 is a 20% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, .. |
|||
Izod Impact, Notched | 0.590 J/cm @Temperature -30.0 °C |
1.11 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® ENH4550 PBT 25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
UBE UBESTA® 3024LU Rigid Black Electronic Grade Nylon 12 Description: UBESTA Nylon 12 has an excellent termite resistance than other plastics. UBESTA contributes as a material for jacket and sheath which lay for telephone and telegram Communication System.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ISO 180-93 |
Wellman Wellpet® MRGF101-GY1 PET, 29% Mineral/Glass Fiber Reinforced Typical data obtained from injection molded test bars, tested dry as molded at 73°F (23°C). Information provided by Wellman, Inc. Engineering Resins Division. |
|||
Izod Impact, Notched | 0.590 J/cm @Thickness 3.17 mm |
1.11 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Entec Hypro™ PPC-T20 Copolymer Polypropylene, 20% Talc Reinforced Information provided by Entec |
|||
Izod Impact, Notched | 0.590 J/cm @Temperature 23.0 °C |
1.11 ft-lb/in @Temperature 73.4 °F |
DAM; ASTM D256 |
DuPont Performance Polymers Zytel® FE3071 NC010 Nylon 66 Zytel® FE3071 NC010 is an intermediate viscosity polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Izod Impact, Notched | 0.590 J/cm @Thickness 3.17 mm |
1.11 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Dry) Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Chem Polymer Chemlon 125-15 MG Nylon 66, 25% Mineral/15% Glass Fiber Reinforced A 25% mineral reinforced, 15% glass fiber reinforced nylon 66 offering excellent rigidity, dimensional stability and tensile strength with improved warpage control in large area parts.Data provided .. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 109 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 446 Glass/Mineral Reinforced, PET Alloy Data provided by the manufacturer, ComAlloy International Company.35% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 617 Nylon 6, Glass/Mineral Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.55% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 520-13G Nylon 66, 13% Glass Reinforced 13% Glass reinforced Nylon 66.Data provided by the manufacturer |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | |
Owens Corning Glass Fiber Reinforced Polypropylene, 20 wt.% glass Polypropylene provides good resistance to acids, alkalis and organic solvents even at higher temperatures. It is, however, soluble in chlorinated hydrocarbons. Data provided by the manufacturer, Ow.. |
|||
Izod Impact, Notched | 0.590 - 0.907 J/cm @Temperature -40.0 - -40.0 °C |
1.11 - 1.70 ft-lb/in @Temperature -40.0 - -40.0 °F |
Average value: 0.730 J/cm Grade Count:3 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Notched | 0.590 J/cm | 1.11 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, at 50% RH
& Data provided by the manufacturer, Amoco Corporation.AMODEL AF-1550 V0 resin is a 50% glass/mineral reinforced, flame retarded polyphthalamide (PPA) that features: high deflection temperature, high .. |