Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ASTM D256 |
SABIC PP 5703P Polypropylene Homopolymer for Injection Molding Product Description: PP 5702P is specially developed for producing rigid injection molded articles for general purpose applications. It gives consistent processability and high gloss in the produc.. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ASTM D256 |
SABIC PP 578P Polypropylene Homopolymer for Injection Molding Product Description: PP 578P is a controlled rheology PP grade of medium molecular weight distribution suitable for injection molding applications. It gives consistent processability, good flow pr.. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® DMX3415M PC Copolymer (Europe-Africa-Middle East) Lexan* DMX3415M is a co-polycarbonate resin with improved scratch and abrasion resistance compared to standard polycarbonate. Lexan* DMX3415M is available in transparent colors. |
|||
Izod Impact, Notched | 0.300 - 7.50 J/cm @Temperature -50.0 - 0.000 °C |
0.562 - 14.1 ft-lb/in @Temperature -58.0 - 32.0 °F |
Average value: 3.76 J/cm Grade Count:89 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Izod Impact, Notched | 0.300 - 0.427 J/cm @Thickness 1.57 - 3.17 mm |
0.562 - 0.800 ft-lb/in @Thickness 0.0618 - 0.125 in |
Average value: 0.642 J/cm Grade Count:2 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Flint Hills P4C6B-194 Polypropylene Homopolymer Features: Antistat, Nucleated. Product does not contain animal derived components. Phthalate-free.Applications: Injection MoldingInformation Provided by Flint Hills Resources |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | 23° C; ASTM D256 |
Flint Hills P4G4K-038 Homopolymer Polypropylene Homopolymer, UL certified, and FDA compliant.Features: Nucleated, antistat, and clarified.Applications: Injection molding: high clarity, housewares, and syringes, for EO sterilization.Former Huntsma.. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ASTM D256 |
LG Chemical LUCEL EC-610B Electrically Conductive POM, 10% Carbon Black Filled LUCEL semi-crystalline acetal copolymer resins are produced by gas phase polymerization. LUCEL resins can be widely accepted as the replacement of thermosets, aluminum and zinc die-casts or other m.. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature 23.0 °C |
0.562 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® GP-2000 General Purpose PBT, Unreinforced, Medium Viscosity LUPOX semi-crystalline thermoplastic PBT resins exhibit properties including high strength, rigidity and good resistance to fatigue and creep at elevated temperatures. Furthermore, LUPOX resins sho.. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ASTM D256-03 |
Ipiranga Petrochem PH 1721 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Izod Impact, Notched | 0.300 - 0.400 J/cm | 0.562 - 0.749 ft-lb/in | ASTM D256 |
Loxim 800 00 HB Polypropylene Compound, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.300 - 0.400 J/cm | 0.562 - 0.749 ft-lb/in | ASTM D256 |
Loxim 820 02C HB Polypropylene Compound, 20% Calcite Filled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | 0.300 - 0.400 J/cm | 0.562 - 0.749 ft-lb/in | ASTM D256 |
Loxim 830 02T HB Polypropylene Compound, 30% Talc Filled, Flame Retardant Information provided by Loxim Industries |
|||
Izod Impact, Notched | >= 0.300 J/cm | >= 0.562 ft-lb/in | Method A; ASTM D 256 |
Karina E 800-35/1-Y-CRB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP WX07423H PBT Health care grade, PTFE and silicone lubricated |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature -30.0 °C |
0.562 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Asia Pacific) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature -30.0 °C |
0.562 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an.. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ASTM D256 |
Unitika M1030E PA6, Dry Nano composite nylonInformation provided by Unitika Ltd. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1058 General Purpose Homopolymer Polypropylene (30% Fiberglass) DescriptionPolyflam® RPP 1058 is a general purpose homopolymer polypropylene flame retardant with a UL-V2 flammability rating and 105°C temperature index at 0.030 in.Information provided by A. Sch.. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ISO 180 |
Wellman Wellamid® T423-BK10 Mineral Reinforced Nylon 6, Heat Stabilized Typical Applications: Lawn and garden equipment, automotive trim, bezels, wheel covers, window frames, gas tank filler housings, brackets, metalized lighting reflectors for automotive, automotive co.. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ RPP 1058 General Purpose Homopolymer Polypropylene (30% Fiberglass) DescriptionPolyflam® RPP 1058 is a general purpose homopolymer polypropylene flame retardant with a UL-V2 flammability rating and 105°C temperature index at 0.030 in.Information provided by A. Sch.. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ASTM D256, Notch |
Cresset Powers Cress-Alon™ NE2740 4% Nano Clay Loaded, 2.7 r.v. Compounding Grade Nylon 6, Dry As Molded Low density, high rigidity, high heat distortion temperature, high retention of mechanical properties under humid conditions, flame retardant, recyclable and environmentally friendly, less glass fib.. |
|||
Izod Impact, Notched | 0.300 - 0.350 J/cm | 0.562 - 0.656 ft-lb/in | UV Postcure; ASTM D256A |
DSM Somos® NeXt LV Grey The second member of the Somos® NeXt family, Somos® NeXt LV Grey delivers the durability and functionality, with a finer resolution of details and faster part processing. This third-generation, hi.. |
|||
Izod Impact, Notched | 0.300 J/cm @Thickness 3.20 mm |
0.562 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Beijing Chemical Industry KAIFA® HN201-G20 PA6 Resin 20% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Izod Impact, Notched | 0.300 J/cm - NB @Temperature -40.0 - -20.0 °C |
0.562 ft-lb/in - NB @Temperature -40.0 - -4.00 °F |
Average value: 2.20 J/cm Grade Count:21 |
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and.. |
|||
Izod Impact, Notched | 0.300 J/cm @Thickness 3.20 mm |
0.562 ft-lb/in @Thickness 0.126 in |
ASTM D256 |
Beijing Chemical Industry KAIFA® 301-G0 PBT Resin Flame retardant, folding enduranceInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Izod Impact, Notched | 0.300 J/cm @Temperature -30.0 °C |
0.562 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL RN0611 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0611 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
Izod Impact, Notched | 0.300 J/cm | 0.562 ft-lb/in | ASTM D256 |
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin U-60 grade Celazole® polybenzimidazole (PBI) resin is a organic polymer which does not burn in air and has high temperature resistance, along with excellent stability to chemicals and hydrolysis. .. |
|||
Izod Impact, Notched | 0.300 - 4.35 J/cm @Temperature -40.0 - 121 °C |
0.562 - 8.15 ft-lb/in @Temperature -40.0 - 250 °F |
Average value: 1.55 J/cm Grade Count:16 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |