Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.800 - 1.40 J/cm² | 3.81 - 6.66 ft-lb/in² | Average value: 1.14 J/cm² Grade Count:17 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
Charpy Impact, Notched | 0.350 - 1.40 J/cm² | 1.67 - 6.66 ft-lb/in² | Average value: 0.836 J/cm² Grade Count:5 |
Overview of materials for Polyphenylene Ether, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ.. |
|||
Charpy Impact, Notched | 0.300 - 1.40 J/cm² @Temperature -40.0 - -30.0 °C |
1.43 - 6.66 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 0.804 J/cm² Grade Count:49 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact, Notched | 0.500 - 1.40 J/cm² | 2.38 - 6.66 ft-lb/in² | Average value: 0.850 J/cm² Grade Count:8 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
Charpy Impact, Notched | 0.500 - 1.40 J/cm² | 2.38 - 6.66 ft-lb/in² | Average value: 0.800 J/cm² Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
Charpy Impact, Notched | 0.410 - 1.40 J/cm² | 1.95 - 6.66 ft-lb/in² | Average value: 0.675 J/cm² Grade Count:4 |
Overview of materials for Nylon 12, Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Graphite Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
Charpy Impact, Notched | 1.26 - 1.40 J/cm² | 6.00 - 6.66 ft-lb/in² | Average value: 1.31 J/cm² Grade Count:3 |
Overview of materials for Nylon 12, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |
|||
Charpy Impact, Notched | 0.280 - 1.40 J/cm² | 1.33 - 6.66 ft-lb/in² | Average value: 0.715 J/cm² Grade Count:11 |
Overview of materials for Nylon 66, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Charpy Impact, Notched | 0.600 - 1.40 J/cm² | 2.86 - 6.66 ft-lb/in² | Average value: 0.830 J/cm² Grade Count:10 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Charpy Impact, Notched | 0.630 - 1.40 J/cm² | 3.00 - 6.66 ft-lb/in² | Average value: 0.826 J/cm² Grade Count:8 |
Overview of materials for Polyphenylene Ether, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 30% Glass Filled". Specific grades with glass content between 25% and 34% are inclu.. |
|||
Charpy Impact, Notched | 1.10 - 1.40 J/cm² | 5.24 - 6.66 ft-lb/in² | Average value: 1.24 J/cm² Grade Count:5 |
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled". Each property range of values reported is .. |
|||
Charpy Impact, Notched | 1.10 - 1.40 J/cm² @Temperature -30.0 - -30.0 °C |
5.24 - 6.66 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.24 J/cm² Grade Count:5 |
Overview of materials for Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether + Styrene-Butadiene Blend, Glass Filled". Each property range of values reported is .. |
|||
Charpy Impact, Notched | 0.0400 - 1.40 J/cm² @Temperature -30.0 - -20.0 °C |
0.190 - 6.66 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.266 J/cm² Grade Count:30 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact, Notched | 0.200 - 1.40 J/cm² | 0.952 - 6.66 ft-lb/in² | Average value: 0.514 J/cm² Grade Count:19 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |
|||
Charpy Impact, Notched | 0.600 - 1.40 J/cm² @Temperature -40.0 - -30.0 °C |
2.86 - 6.66 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 0.850 J/cm² Grade Count:7 |
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Charpy Impact, Notched | 0.900 - 1.40 J/cm² | 4.28 - 6.66 ft-lb/in² | Average value: 1.11 J/cm² Grade Count:8 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |
|||
Charpy Impact, Notched | 0.900 - 1.40 J/cm² @Temperature -30.0 - -30.0 °C |
4.28 - 6.66 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.08 J/cm² Grade Count:6 |
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% .. |
|||
Charpy Impact, Notched | 0.600 - 1.40 J/cm² | 2.86 - 6.66 ft-lb/in² | Average value: 0.929 J/cm² Grade Count:32 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |
|||
Charpy Impact, Notched | 0.800 - 1.40 J/cm² | 3.81 - 6.66 ft-lb/in² | Average value: 1.01 J/cm² Grade Count:30 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |