Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.120 - 1000 J/cm² | 0.571 - 4760 ft-lb/in² | Average value: 1.40 J/cm² Grade Count:83 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Charpy Impact, Notched | 0.300 - 1000 J/cm² | 1.43 - 4760 ft-lb/in² | Average value: 0.664 J/cm² Grade Count:161 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Charpy Impact, Notched | 0.200 - 1000 J/cm² | 0.952 - 4760 ft-lb/in² | Average value: 1.11 J/cm² Grade Count:124 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Charpy Impact, Notched | 0.600 - 1000 J/cm² | 2.86 - 4760 ft-lb/in² | Average value: 2.75 J/cm² Grade Count:13 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Charpy Impact, Notched | 0.200 - 1000 J/cm² | 0.952 - 4760 ft-lb/in² | Average value: 1.55 J/cm² Grade Count:16 |
Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |
|||
Charpy Impact, Notched | 0.400 - 1000 J/cm² | 1.90 - 4760 ft-lb/in² | Average value: 3.09 J/cm² Grade Count:31 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Charpy Impact, Notched | 0.100 - 1000 J/cm² | 0.476 - 4760 ft-lb/in² | Average value: 1.21 J/cm² Grade Count:161 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Charpy Impact, Notched | 0.370 - 1000 J/cm² | 1.76 - 4760 ft-lb/in² | Average value: 2.01 J/cm² Grade Count:64 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Charpy Impact, Notched | 0.420 - 1000 J/cm² | 2.00 - 4760 ft-lb/in² | Average value: 0.770 J/cm² Grade Count:5 |
Overview of materials for Nylon 11, Cable Sheathing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Cable Sheathing Grade". Each property range of values reported is minimum and maximum values o.. |
|||
Charpy Impact, Notched | 1.00 - 1000 J/cm² | 4.76 - 4760 ft-lb/in² | Average value: 2.00 J/cm² Grade Count:7 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Charpy Impact, Notched | 0.300 - 1000 J/cm² | 1.43 - 4760 ft-lb/in² | Average value: 3.31 J/cm² Grade Count:11 |
Overview of materials for Nylon 6, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Charpy Impact, Notched | 3.00 - 1000 J/cm² | 14.3 - 4760 ft-lb/in² | Average value: 6.73 J/cm² Grade Count:48 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a.. |
|||
Charpy Impact, Notched | 5.00 - 1000 J/cm² | 23.8 - 4760 ft-lb/in² | Average value: 7.00 J/cm² Grade Count:13 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a.. |
|||
Charpy Impact, Notched | 0.200 - 1000 J/cm² | 0.952 - 4760 ft-lb/in² | Average value: 0.766 J/cm² Grade Count:239 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Charpy Impact, Notched | 0.200 - 1000 J/cm² | 0.952 - 4760 ft-lb/in² | Average value: 0.300 J/cm² Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |
|||
Charpy Impact, Notched | 0.130 - 1000 J/cm² | 0.619 - 4760 ft-lb/in² | Average value: 4.67 J/cm² Grade Count:31 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |
|||
Charpy Impact, Notched | 0.300 - 1000 J/cm² | 1.43 - 4760 ft-lb/in² | Average value: 1.82 J/cm² Grade Count:181 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |