Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 S20 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL B63 HS-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 L-HS-GV15 Nylon 6 for injection molding, 15% glass fiber reinforced Nylon 6 for injection molding, improved fluidity, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa SINKRAL B633/E ABS, Impact & Heat Stabilized Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,EG,105-04-25-20 High impact extrusion grade with excellent stiffness, good processability and high thermal stabili.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
|
Polimeri Europa SINKRAL B813 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-04-35-15 Injection moulding grade, providing very high impact resistance, even at low temperatures. Used as.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | |
Ineos ABS Lustran® H607AS Contains antistatic additives,Property data per ISO test methods. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179 |
Iran Petrochemical (PCC) BL8 HM 7745 High Density Polyethylene BL8 (HM 7745) is a high density polyethylene with Butene-1 as comonomer.Applications: for heating oil storage tanks, large containers for various chemicals.Information provided by Iran Petrochemical.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | |
Ineos ABS Lustran® Elite HH 1827 Key Features:UnfilledHeat stabilized or stable to heatSuitable processing methods:Injection molding |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 218 V40 PA66, 40% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 40% of glass fiber, heat stabilized for injection molding.Available in: Asia Pacific, Europe and North AmericaProduct Applications: TECHNYL A 218 V40 is .. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 218 V43 Black 21 N PA66, 43% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 43% of glass fiber, heat stabilized, for injection molding.Available in: North AmericaProduct Applications: TECHNYL® A 218 V43 is used in all sectors .. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYLSTARâ„¢ S 216 V35 PA6, 35% glass filled, Conditioned Description: TECHNYLSTAR polyamide, reinforced with 35% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North AmericaProduct Applications.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Ultem HATX100 PEI+PCE Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature 23.0 °C |
9.04 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Ultem HATX100 PEI+PCE (Asia Pacific) Higher impact, high flow Polyetherimide blend. ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO Data |
Styron Magnum™ 9010 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS (Asia Pacific) NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL PKN4775 PPE+PS (Europe-Africa-Middle East) PPE+PS blend. Opaque. FDA compliant in limited colors. High heat. Modulus at elevated temperature. Good ESCR performance. Thin wall extrusion and injection molding. Typical applications include pack.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL PX1134 PPE+HIPS (Europe-Africa-Middle East) NORYL PX1134 is an unfilled material with a Vicat B/120 of 120°C according ISO 306. NORYL PX1134 offers improved impact performance to meet the standard ECE dashboard impact tests in the automoti.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 218HP V30 Black 21N PA66, 30% glass fiber, Conditioned Provisional datasheet - Product in developmentDescription: Polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYLÂ.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics NORYL EXNL0303 PPE+HIPS (Asia Pacific) EXNL0303 is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nor.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | dry; ISO 179 |
Ter Hell Plastic Terez® ABS 3320 A UV Acrylonitrile Butadiene Styrene Rapid flowing ABS with high impact strength, antistatic agent and UV stabilizer.Application: For all kinds of injection molding thin-walled parts.Information provided by Ter Hell Plastic GMBH. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® TW200F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact, Notched | 1.90 J/cm² @Temperature -30.0 °C |
9.04 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DSM Stanyl® TW241F12 (COND) Nylon 46 60% Glass Reinforced, Heat Stabilized, High Flow (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® LV-30H FWA black 9225 PA12-GF30 Product description: Grilamid LV-30H FWA black 9225 is a 30 % glass fiber reinforced, heat stabilized polyamide12 injection molding grade with the following special features: Stiffness combined with.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® XE 4104 nat PA610-GF40 Product description: Grilamid XE 4104 natural is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw materia.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 73G45 BK263 Nylon 6
(Unverified Data**) 45% Glass Reinforced Polyamide 6 Zytel 73G45 BK263 is a 45% glass fiber reinforced black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | |
Arkema Group Rilsan® BMN P20 D Nylon 11 (Dry) Designation ISO 1874-PA11-P,MR,12-004Flexible grade for injection molding. Available colors: black and natural. Mold release agent.Outstanding working properties. Easy filling of the mold due to its.. |
|||
Charpy Impact, Notched | 1.90 J/cm² | 9.04 ft-lb/in² | 1eA; ISO 179 |
Azoty Tarnow™ TARFLEN SM-2 PTFE Non Free Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |