Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.500 J/cm² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB POLYfill PP HBK15030 Polypropylene, Multifiller High Gloss Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.500 J/cm² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS (Asia Pacific) Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro.. |
|||
Charpy Impact, Notched | 0.500 J/cm² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CX7010 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7010 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0. Excellent flow combined with good balance of pro.. |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 SG-GV 2010 Nylon 6.6 for injection molding, 20% mineral filled and 10% glass fiber reinforced Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics GELOY FXW749SK ASA Sparkle VisualFx ASA Resin - Weatherable |
|||
Charpy Impact, Notched | 0.500 J/cm² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polykemi AB SCANAMID 66 A12^ F20 FR6 Nylon 66, Glass Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179-1/1eA |
Quadrant EPP Ketron® CA30 PEEK + carbon fibres, extruded (ISO Data) This 30 % carbon fibre reinforced grade combines even higher stiffness, mechanical strength and creep resistance than Ketron PEEK-GF30 with an optimum wear resistance. Moreover, compared with unrein.. |
|||
Charpy Impact, Notched | 0.500 J/cm² @Temperature -40.0 °C |
2.38 ft-lb/in² @Temperature -40.0 °F |
ISO 179/1eA |
DuPont Performance Polymers Hytrel® 7246HS BK320 TPC-ET
(Unverified Data**) Hytrel® 7246HS BK320 is a high modulus, heat stabilized, black grade with nominal hardness of 72D.Information provided by DuPont |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | DIN 53453 |
Nilit FRIANYL A63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced Nylon 6.6 for injection molding (good conductive and electrostatic properties).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 1106-7940/GY/EM Polyether imide, unreinforced, laser markable Applications: High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.High dimensionally stable precision parts.Information provided by Le.. |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179/1eA |
Kuraray Genestarâ„¢ N1002A-M41 Nylon Low friction unreinforced injection grade. Main Features:Low friction coefficientLow wearExamples of applications are:Friction and wear applicationGear and wheel |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | |
LATI Larpeek 10 K/20 PEEK, 20% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | |
LATI Latan 13 S/15 POM, 15% Glass Bead Reinforced Polyoxymethylene (POM) based compound. Glass beads. Medium viscosity. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation pro.. |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | |
LATI Latilub 62-15ST PA6 Self-lubricating product based on Polyamide 6 (PA6). Silicone / PTFE.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Term.. |
|||
Charpy Impact, Notched | 0.500 J/cm² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL V090 PPE+HIPS (Europe-Africa-Middle East) NORYL V090 is an unfilled, flame retardant material with a Vicat B/120 of 95 °C according ISO 306. NORYL V090 is V0 at 2.0 mm and V1 at 1.6 mm according UL94 and halogen free according VDE/DIN 47.. |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® 815F PBT+PET PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYL® A 205F PA66, DRY Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Charpy Impact, Notched | 0.500 J/cm² @Temperature -20.0 °C |
2.38 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis BorECO™ BA212E Polypropylene Block Copolymer for Non-Pressure Pipes BorECO BA212E is a high molecular weight, low melt flow rate polypropylene block copolymer with very high stiffness and impact strength.BorECO BA212E is recommended for solid wall and structured wal.. |
|||
Charpy Impact, Notched | 0.500 J/cm² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Borealis Daplen™ EE015U TPO Compound Daplen EE015U is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE015U is a material with excellent impact /stiffness ratio. Thanks to its low th.. |
|||
Charpy Impact, Notched | 0.500 J/cm² @Temperature 30.0 °C |
2.38 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4180 black 9992 PA1010 Product description: Grilamid XE 4180 black 9992 is a unreinforced, high viscosity, plasticized, high impact resistant polyamide 1010 (PA1010) extrusion grade. Grilamid XE 4180 black 9992 is highly .. |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Delrin® 500TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500TL is a medium viscosity acetal homopolymer resin containing 1.5% Teflon PTFE Micropowder. It is desi.. |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179/IeA |
Addiplast Addilene J 520 M40 Polypropylene Copolymer Mineral reinforced, improved rigidityInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179/IeA |
Addiplast Addinyl A2 E Flame Retardant Nylon 66 Flame retardant, halogen freeInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.500 J/cm² | 2.38 ft-lb/in² | ISO 179-1eA |
Barlog Plastics KEBAFORM C 3090(K) POM Copolymer, 27% glass fiber reinforced POM-GF27Information provided by BARLOG plastics GmbH. |
|||
Charpy Impact, Notched | 0.500 - 0.800 J/cm² @Temperature -40.0 - -30.0 °C |
2.38 - 3.81 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 0.653 J/cm² Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |
|||
Charpy Impact, Notched | 0.500 J/cm² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Valox® VX4915 ASA+PBT (Europe-Africa-Middle East) 15% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |