Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.400 - 0.450 J/cm² | 1.90 - 2.14 ft-lb/in² | Injection; ISO 179/1eA |
Raschig Group 2557 AMC Polyester Glass fiber reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, exceptional processability with short cycle time and low .. |
|||
Charpy Impact, Notched | 0.350 - 0.450 J/cm² @Temperature 23.0 °C |
1.67 - 2.14 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eA |
Raschig Group 5562 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Charpy Impact, Notched | 0.350 - 0.450 J/cm² @Temperature 23.0 °C |
1.67 - 2.14 ft-lb/in² @Temperature 73.4 °F |
Injection; ISO 179/ 1eA |
Raschig Group 5563 DAP Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona.. |
|||
Charpy Impact, Notched | 0.250 - 0.450 J/cm² | 1.19 - 2.14 ft-lb/in² | Compression; ISO 179/1eA |
Raschig Group 6551 DAIP Diallyl Phthalate (DAP), Cast, Mineral Filler Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi.. |
|||
Charpy Impact, Notched | 0.150 - 0.450 J/cm² | 0.714 - 2.14 ft-lb/in² | Average value: 0.211 J/cm² Grade Count:32 |
Overview of materials for Phenolic, Novolac, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral Filled". Each property range of values reported is minimum and maximum values.. |
|||
Charpy Impact, Notched | 0.281 - 0.450 J/cm² | 1.34 - 2.14 ft-lb/in² | Average value: 0.357 J/cm² Grade Count:3 |
Overview of materials for Phenolic/Rubber; Molded This property data is a summary of similar materials in the MatWeb database for the category "Phenolic/Rubber; Molded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Charpy Impact, Notched | 0.350 - 0.450 J/cm² | 1.67 - 2.14 ft-lb/in² | ISO 179 |
Vyncolit 4451 XB Novolac Phenolic Organic and mineral filled phenolic molding compound with excellent mechanical properties (highest notched impact strength).USES: Fuse holders, brush holders, circuit breakers, automotive ignition a.. |