Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CX5430 PC+ABS (Asia Pacific) Cycoloy* resin CX5430 is a general purpose PC/ABS blend developed for thin wall applications requiring weld line strength, high flow and impact together with a good balance of other properties. |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Asia Pacific) Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 23.0 °C |
19.0 ft-lb/in² @Temperature 73.4 °F |
DIN 53453 |
Qualchem Danamid AFES-21 Polyamide 66 Impact resistant, dryInformation provided by Qualchem Zrt. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® LUX2910 PC (Asia Pacific) Global grade. LEXAN LUX2910 is an injection moulding grade especially designed for manufacturing optical parts requiring superior flow properties combined with very high transmission and color stabi.. |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® LUX2910T_ PC (Europe-Africa-Middle East) Global grade. LEXAN LUX2910T is an injection moulding grade especially designed for manufacturing optical parts requiring superior flow properties combined with very high transmission and color stab.. |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® OQ1022 PC (Asia Pacific) Standard Flow OQ Resin |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS (Asia Pacific) Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che.. |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CX7211 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7211 PC/ABS resin is a non-filled, injection moldable grade which has UL 94 rating at 2.5 mm 5VA. Cycoloy CX7211 resin provides all color options and features an excellent balance of flo.. |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | |
Ineos ABS Lustran® 446 Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Injection molding |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Valox® 357X PBT (Europe-Africa-Middle East) VALOX 357X is an impact modified, flame retarted PBT+PC blend. Applications like bobbins, switches and enclosures. |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Asia Pacific) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | ISO Data, Low Temp |
Styron CALIBRE™ IM 401 11 Polycarbonate, Impact Modified CALIBRE® IM401 series resins are impact modified, UL listed polycarbonate resins which contain mold release. CALIBRE IM401 polycarbonate resins exhibit an excellent balance of impact strength and.. |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | ISO 179/1eA |
Borealis Beta-PPR™ RA7050-GN Polypropylene-Random-Copolymer for Pressure Pipe Systems Beta-PPR RA7050-GN is a PP-RCT, a Polypropylene-Random-Copolymer with an enhanced Crystalline structure brought about by a special ß-nucleation and with an improved Temperature resistance. Proof o.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature -30.0 °C |
19.0 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Covestro Makroblend® DP UT6005 Polycarbonate + PBT, Impact Grade Developmental product(PC+PBT)-blendimpact modifiedeasy releaseinjection molding grade Makroblend DP UT6005* offers an exceptional low-temperature impact strength, good flowability and excellent ch.. |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® GVL-6H nat PA*-GF60 Product description: Grivory GVL-6H natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H na.. |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® L 20 W 20 grey 9280 PA12 Product Description: Grilamid L 20 W 20 grey 9280 is a semiflexible plasticized medium viscosity polyamide 12 (PA12) extrusion grade. Grilamid L 20 W 20 grey 9280 is heat stabilized. The main featur.. |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® TSGL-60/4 black 9833 PA666-GF60 Product description: Grilon TSGL-60/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black is characterized by the following key-p.. |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® TSGL-60/4 black 9839 PA666-GF60 Product description: Grilon TSGL-60/4 black 9839 is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black 9839 is characterized by the foll.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 30.0 °C |
19.0 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-60/4 black 9839 PA666-GF60 Product description: Grilon TSGL-60/4 black 9839 is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black 9839 is characterized by the foll.. |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® XE 4071 nat PA612-I Product description: Grilamid XE 4071 NATURAL is an unreinforced impact modified high viscosity polyamide 612 (PA612) extrusion grade with superior hydrolysis and heat resistance. Compared to standa.. |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® FG53 NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® GVL-6H black 9839 PA*-GF60 Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac.. |
|||
Charpy Impact, Notched | 4.00 J/cm² @Temperature 30.0 °C |
19.0 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GVL-6H black 9839 PA*-GF60 Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac.. |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | After conditioning at 23°C/50%RH; ISO 179/Af |
Arkema Group Orgalloy® LE 60XV Polyamide 6 Alloy Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | ISO 179/IeA |
Addiplast Addilene J 370 Polypropylene Copolymer High impact strength, high elongation at breakInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | ISO 179 |
BASF Ultramid® HPN 9350 HS PA6 (Dry) Ultramid HPN 9350 HS is a flexible, heat stabilized, impact modified PA6 extrusion grade resin. It possesses a balance of performance properties such as good flexibility, toughness and abrasion res.. |
|||
Charpy Impact, Notched | 4.00 J/cm² | 19.0 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addinyl PMD 20143 Nylon 6 High impact resistanceInformation provided by Addiplast. |