Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1... |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 S10 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 103 PC (Europe-Africa-Middle East) LEXAN 103 is a high viscosity U.V. stabilized multi purpose grade. LEXAN 103 is available in transparent, translucent and opaque colours. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL4019 PC (Asia Pacific) Lexan* EXL4019 is an opaque 9% Glass Fiber (GF) reinforced polycarbonate (PC) siloxane copolymer resin for injection molding (IM) applications requiring improved stiffness. This resin also offers im.. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® EXL4419 PC Copolymer Lexan* EXL4419 polycarbonate (PC) siloxane copolymer resin is a 9% Glass Fiber (GF) reinforced opaque injection molding (IM) grade. This medium flow resin offers much higher ductility, improved rele.. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPH4504 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Asia Pacific) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® OQ3820 PC (Europe-Africa-Middle East) High Viscosity, UV-stabilized grade for ophthalmic lenses. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX2432T PC Copolymer (Asia Pacific) Medium viscosity PC copolymer with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX2531T PC Copolymer (Asia Pacific) Transparent weatherable PC copolymer for blowmolding/extrusion. |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | DIN 53453 |
Nilit FRIANYL B63 W-GV25 Nylon 6 for injection molding, 25% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.50 - 3.50 J/cm² @Temperature -20.0 - -20.0 °C |
7.14 - 16.7 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 1.62 J/cm² Grade Count:2 |
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO Data, Low Temp |
Styron Pulse® 600 ABS + Polycarbonate PULSE® 600 Engineering resin is designed to offer a superior balance of properties between impact strength, heat resistance and processability. It offers excellent processability, medium heat res.. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GS 30 HWUVCP 30% Glass Sphere Filled Nylon 6, UV Stabilized Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature 30.0 °C |
7.14 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® BZ 3 PA6 Information provided by EMS Grivory |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® GV-5H EF nat PA*-GF50 Product description: Grivory GV-5H EF natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam.. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6600 MF30 HWCP 30% Milled Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature 30.0 °C |
7.14 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GVS-5H nat PA*-GF50 Product description: Grivory GVS-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide.. |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® GVX-65 H nat PA*-GF65 Product description: Grivory GVX-65H natural is a 65% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyami.. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature 30.0 °C |
7.14 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GVX-65 H nat PA*-GF65 Product description: Grivory GVX-65H natural is a 65% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyami.. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature 30.0 °C |
7.14 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® LV-50H FWA nat PA12-GF50 Product description: Grilamid LV-50H FWA natural is a 50 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature 30.0 °C |
7.14 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 4116 black 9288 PA1010-GF55 Product description: Grilamid XE 4116 black 9288 is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, paint.. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® FG70G50HSLA BK309 Nylon 66
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO 179 |
BASF Ultramid® 8234G HS BK 102 44% Glass Filled PA6 (Dry) Description Ultramid 8234G HS BK-102 is heat stabilized, pigmented black, 44% glass reinforced PA6 injection molding compound offering the highest level of strength, stiffness, high temperature perf.. |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO179 |
Beijing Chemical Industry KAIFA® M104N MPPO Resin High flame retardant, Good flowInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addinyl C2 Nylon 66/6 Unreinforced, medium viscosityInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 1.50 J/cm² | 7.14 ft-lb/in² | ISO 179 / 1eA |
Asahi Kasei Tenac® SH210 Homopolymer Acetal Resin Super high-impact grade; highest molecular weight category.Information provided by Asahi Kasei Corporation. |
|||
Charpy Impact, Notched | 1.50 J/cm² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® ML3485 PC (Europe-Africa-Middle East) LEXAN ML3485 is a low viscosity grade exhibiting an improved ductility over standard polycarbonate grades at equal flow. |