Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179/1eA |
Nilit FRIANYL A63 GV30 Nylon 6.6 for injection molding, 30% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 123R PC (Europe-Africa-Middle East) LEXAN 123R is a low viscosity multi purpose U.V. stabilized grade and contains a release agent to ensure easy processing. LEXAN 123R is available in transparent, translucent and opaque colours. |
|||
Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HPS1R PC Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, e-beam and gamma sterilizable. Cont.. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® LI1813R PC (Europe-Africa-Middle East) Low-viscosity multi-purpose PC having low levels of ionics species. UV-stabilized. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® 4704 PC (Europe-Africa-Middle East) High heat resistant polycarbonate copolymer, provides of 165 C at 1.82 MPa. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with bi.. |
|||
Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® HP1R PC High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains a higher amount.. |
|||
Charpy Impact, Notched | 1.20 - 1.50 J/cm² @Temperature -30.0 - -30.0 °C |
5.71 - 7.14 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 1.38 J/cm² Grade Count:2 |
Overview of materials for Nylon 612, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Impact Modified". Each property range of values reported is minimum and maximum values of app.. |
|||
Charpy Impact, Notched | 1.20 - 2.50 J/cm² | 5.71 - 11.9 ft-lb/in² | Average value: 1.84 J/cm² Grade Count:21 |
Overview of materials for Nylon 12, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |
|||
Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/SI/2-2 Polyamide 66, with glass fiber, PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Valox® 4031 PBT (Europe-Africa-Middle East) VALOX 4031 is a 30% high strength glass fibre reinforced PBT injection moulding resin with excellent strength, stiffness and heat resistance. Applications: appliance handles, spotlights, electric mo.. |
|||
Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
ISO 179/2C |
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Valox® IQNH4565 PBT (Asia Pacific) Valox* iQNH4565 resin is a non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 29% based on EPEAT.. |
|||
Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | dry; ISO 179 |
Ter Hell Plastic Terez® PA 6 7500 TF 20 GF 20 Polyamide 6, 20% PTFE chemically bonded 20% glass fiber reinforced Description: Medium viscosity PA 6, 20% PTFE chemically bonded and 20% glass fiber reinforced, good flowability, good impact resistance and bright natural color.Application: For molding parts with.. |
|||
Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® BG-15 HM PA6-GF15 Product description: Grilon BG-15 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 15% glass fibers. Grilon BG-15 HM has the following important prop.. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature 30.0 °C |
5.71 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® BG-40 HM PA6-GF40 Product description: Grilon BG-40 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 40% glass fibers. Grilon BG-40 HM has the following important prop.. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GVS 10/30 HWCP 10% Glass Fiber and 30% Glass Sphere Nylon 6, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® HT3Z black 9564 PA* Product description: Grivory HT3Z is an unreinforced and impact resistant, engineering thermoplastic based on semi crystalline partially aromatic copolyamide. This Grivory HT product is partially ba.. |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature 30.0 °C |
5.71 ft-lb/in² @Temperature 86.0 °F |
conditioned; ISO 179/1eU |
EMS-Grivory Grivory® TSG-50 FA PA666-GF50 Information provided by EMS Grivory |
|||
Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179-2 |
Denka MALECCA K-510 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66
(Unverified Data**) 32% Mineral Reinforced Toughened Polyamide 66 Minlon 12TA BKB124 is a 32% mineral reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont P.. |
|||
Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 8018HS BKB085 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 8018HS BKB085 is a 14% glass reinforced toughened heat stabilized black polyamide 66 resin.Information provided by DuPont Performanc.. |
|||
Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | 50%RH; ISO 179/1eA |
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612 33% Glass Reinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature -30.0 °C |
5.71 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 45% Glass Reinforced PPA High Performance Polyamide Zytel HTN51G45HSL BK083 is a 45% glass reinforced heat stabilized lubricated high performance polyamide resin. It is also a PPA resin.Information .. |
|||
Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® HTN 54G35HSLR BKB336 Polyphthalamide (PPA) 35% Glass Reinforced laser markable PPA High Performance Polyamide Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 1.20 J/cm² @Temperature 23.0 °C |
5.71 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000 GV 25 HWCP 25% Glass Fiber Nylon 6, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® TR XE 4139 black 9231 PA* Product description: Grilamid XE 4139 black 9231 is an amorphous thermoplastic polyamide based on aliphatic, cycloaliphatic and aromatic monomers. Grilamid XE 4139 black 9231 contains a processing a.. |
|||
Charpy Impact, Notched | 1.20 J/cm² | 5.71 ft-lb/in² | ISO 179/1eA |
Polyplastics Duracon® SF-10 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |