Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Zytel® HTN 54G35HSLR BKB336 Polyphthalamide (PPA)

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 40% Glass Fiber Reinforced
Manufacturer DuPont Performance Polymers
Trade Name Zytel® HTN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Zytel® HTN 54G35HSLR BKB336 Polyphthalamide (PPA).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
35% Glass Reinforced  laser markable PPA  High Performance Polyamide  Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
DAM; ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 175 MPa
25400 psi
DAM; ISO 527-1/-2
Elongation at Break 3.1 %
3.1 %
DAM; ISO 527-1/-2
Tensile Modulus 10.5 GPa
1520 ksi
DAM; ISO 527-1/-2
Charpy Impact Unnotched 9.00 J/cm²
42.8 ft-lb/in²
DAM; ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²
5.71 ft-lb/in²
DAM; ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 256 °C
493 °F
DAM; ISO 75-1/-2
Descriptive Properties Value Comments
Part Marking Code >PA-IGF35<
ISO 11469
>PPA-IGF35<
SAE J1344
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Special Characteristics Heat stabilised or stable to heat
Users viewing this material also viewed the following: