Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | ISO 179 |
Nilit Polynil® C50L Externally Lubricated PA66/6 Description: Polynil C50L shows better surface finish, flow and elongation than a comparable homopolymer. Key characteristics: Excellent flowHigh elongationGood impact strengthGood overall mechanica.. |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | |
Polimeri Europa EDISTIR PD RK4514H High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,M,093-06-07-23 UL94 V-2, polybromodiphenylether (PBBE) free, antimony free, HIPS satisfying at 960°C the glow wire test.. |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature -30.0 °C |
3.09 ft-lb/in² @Temperature -22.0 °F |
|
Ineos ABS Lustran® LGA-SF
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquir.. |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | ISO 179 1eA |
Lehmann & Voss LUVOCOM® 1105-7442 PEEK, with carbon fiber, easy flowing Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi.. |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | ISO 179/1eA |
Lucite International Diakon® CRG812 Acrylic Polymer, Toughened Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness. The grades in the Diakon® series can be processed b.. |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | |
LATI Latiohm 87/26-06 PD01-V1 PC, Flame Retardant Semiconductive/dissipative product based on Polycarbonate (PC). UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Availability: Africa & Middle East; Asia .. |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | ISO 179/1eA |
Solvay TECHNYLSTARâ„¢ S 218 MT PA6, 40% mineral filled, Conditioned Description: TechnylStar Polyamide, 40% mineral filled, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific and North AmericaProduct Appli.. |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature -20.0 °C |
3.09 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Borpact™ SG321MO Polypropylene Random Heterophasic Copolymer for Injection Molding Borpact SG321MO is a specially designed modified relatively soft and transparent polypropylene random heterophasic copolymer intended for injection molding. Borpact SG321MO has excellent flow, is f.. |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature 23.0 °C |
3.09 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Unipetrol PE HD LITEN® MB 68 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | ISO 179 |
Total PPH 4042 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4042 is a nucleated homopolymer.ApplicationATOFINA Polypropylene PPH 4042 has been developed for extrusion-thermoforming, providing improved rigidity and impact resistance .. |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | ISO 179/1eA |
DuPont Performance Polymers Delrin® 911DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Low Viscosity Acetal Homopolymer Delrin 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less shrinka.. |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | Conditioned; ISO 179/IeA |
Addiplast Addilene PMD 50272 Flame Retardant Polypropylene Flame retardant, high rigidityInformation provided by Addiplast. |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | ISO 179-1eA |
Barlog Plastics KEBAPEAK XC1730 PEEK; 30% carbon fiber reinforced PEEK-CF30Information provided by BARLOG plastics GmbH. |
|||
Charpy Impact, Notched | 0.650 J/cm² @Temperature -30.0 °C |
3.09 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
BASF Ultrason® E 2010 C6 30% Carbon Filled Carbon fibers and Ultrason® two partners with good properties. The combination of carbon fibers with the amorphous high-temperature plastic Ultrason® guarantees mechanical properties for temperatu.. |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | ISO 179/1eA |
BASF Ultrason E 2010 PES Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | DIN 53453 |
3A Composites Core Materials AIREX® R63.140 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable.. |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | ISO 179/1eA |
Radici Heraform® R 1300 Acetal Copolymer Easy flowing grade for injection molding of thin-walled parts with high mechanical properties.Information provided by Radici group. |
|||
Charpy Impact, Notched | 0.650 J/cm² | 3.09 ft-lb/in² | ISO 179/1eA |
Radici Heraform® R 900 Acetal Copolymer Standard grade for injection molding of details with high mechanical requirement.Information provided by Radici group. |