Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.130 - 0.200 J/cm² | 0.619 - 0.952 ft-lb/in² | Injection; ISO 179/1eA |
Raschig Group MELOPAS® 6605 MP Melamine Cellulose reinforced Melamine molding compound. Very good electrical properties, excellent surface hardness, good mechanical strength and heat resistance, good wear and UV-stability, good gliding be.. |
|||
Charpy Impact, Notched | 0.130 - 0.150 J/cm² | 0.619 - 0.714 ft-lb/in² | Injection and Compression; ISO 179/ 1eA |
Raschig Group MELOPLAS® 2500 MF Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al.. |
|||
Charpy Impact, Notched | 0.130 - 1.70 J/cm² @Temperature -30.0 - 10.0 °C |
0.619 - 8.09 ft-lb/in² @Temperature -22.0 - 50.0 °F |
Average value: 0.367 J/cm² Grade Count:85 |
Overview of materials for Polypropylene, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Molded". Each property range of values reported is minimum and maximum values of appropri.. |
|||
Charpy Impact, Notched | 0.130 J/cm² @Temperature 23.0 °C |
0.619 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ PF 31.9 Phenolic Formaldehyde Resin, Ammonia Free
(discontinued **) Phenolic molding compound, mainly organically filled, ammonia free, standardized molding compound.Application areas: Parts for electrical and telecommunications technology, motor vehicle ignition sy.. |
|||
Charpy Impact, Notched | 0.130 J/cm² @Temperature 23.0 °C |
0.619 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1/2 eA |
Hexion Bakelite™ PF 13591 Phenolic Formaldehyde Resin, High Surface Quality, UL Listed
(discontinued **) Phenolic molding compound, mainly organically filled, very soft flow for large molds, UL listed molding compound 1.5 mm/V-1 (BK), 3.0 mm/V-0 (BK).Application areas: Pan handles, various applications.. |
|||
Charpy Impact, Notched | 0.130 - 0.530 J/cm² | 0.619 - 2.52 ft-lb/in² | Average value: 0.363 J/cm² Grade Count:6 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Charpy Impact, Notched | 0.130 J/cm² | 0.619 ft-lb/in² | |
LATI Latigray 52/11-01 CX/70 PP Homopolymer Radiopaque compound based on Polypropylene homopolymer (PPh). Special mineral filler.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Charpy Impact, Notched | 0.130 J/cm² | 0.619 ft-lb/in² | ISO 179-1 |
Vyncolit TX10916 Graphite Filled Novolac Phenolic Novolac resin based, graphite filled compound used for low friction applications where dimensional stability is required.Information provided by Sumitomo Bak North America, Inc. |
|||
Charpy Impact, Notched | 0.130 J/cm² @Temperature -30.0 °C |
0.619 ft-lb/in² @Temperature -22.0 °F |
|
BASF Novolen® 3248 TC Polypropylene Easy-flowing grade containing nucleating and antistatic agents for transparent injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Charpy Impact, Notched | 0.130 J/cm² | 0.619 ft-lb/in² | DIN 53453 |
3A Composites Core Materials AIREX® R82.80 High Performance Structural Foam AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver.. |
|||
Charpy Impact, Notched | 0.130 J/cm² | 0.619 ft-lb/in² | |
LATI Latimass 52/11-01 D020 PP Homopolymer Specific density compound based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Charpy Impact, Notched | 0.130 J/cm² | 0.619 ft-lb/in² | |
LATI Latimass 52/11-04 D008 PP Homopolymer Specific density compound based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Charpy Impact, Notched | 0.130 J/cm² | 0.619 ft-lb/in² | |
LATI Latimass 52/35-04 D009 PP Homopolymer Specific density compound based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |
|||
Charpy Impact, Notched | 0.130 J/cm² | 0.619 ft-lb/in² | |
LATI Latimass 53-04 D008 PP Homopolymer, Impact Modified Specific density compound based on Polypropylene homopolymer (PPh), impact modified. Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation.. |
|||
Charpy Impact, Notched | 0.130 J/cm² | 0.619 ft-lb/in² | |
LATI Latiohm 66-10 H2 CNT CE/10 PA66, 10% Mineral Fiber Reinforced, Heat Stabilized Semiconductive/dissipative product based on Polyamide 66 (PA66). Heat stabilized. Carbon nanotubes. Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ame.. |
|||
Charpy Impact, Notched | 0.130 - 1000 J/cm² | 0.619 - 4760 ft-lb/in² | Average value: 4.67 J/cm² Grade Count:31 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |