Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Cycolac® INP562 ABS+SAN SABIC INP562 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C |
SABIC Innovative Plastics Cycolac® INP563 ABS SABIC INP563 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C |
SABIC Innovative Plastics Cycolac® INP564 ABS SABIC INP564 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Cycolac® INP564 ABS+SAN SABIC INP564 provides compatibility with a wider range of ABS grades than many color concentrate bases; allows better dispersion than pellets; allows concentrate manufacturers to produce both pellet.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
ISO 179/2C |
SABIC Innovative Plastics Cycolac® INP630 ABS INP630 is a specialty polymer that increases the service temperature of products. Can be used with a impact modifier to provide impact strength as well as high heat resistance.
Provides excellent hi.. |
|||
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Cycolac® INP630 ABS+SAN INP630 is a specialty polymer that increases the service temperature of products. Can be used with a impact modifier to provide impact strength as well as high heat resistance. Provides excellent hi.. |
|||
Charpy Impact, Notched | 0.100 - 0.200 J/cm² | 0.476 - 0.952 ft-lb/in² | Compression; ISO 179/1eA |
Raschig Group RALUPOL® 2100 UP Polyester Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta.. |
|||
Charpy Impact, Notched | 0.100 - 1.80 J/cm² | 0.476 - 8.57 ft-lb/in² | Average value: 0.967 J/cm² Grade Count:6 |
Overview of materials for PET + PBT Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PET + PBT Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Charpy Impact, Notched | 0.100 J/cm² - NB | 0.476 ft-lb/in² - NB | Average value: 1.18 J/cm² Grade Count:147 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Charpy Impact, Notched | 0.100 - 2.50 J/cm² | 0.476 - 11.9 ft-lb/in² | Average value: 0.992 J/cm² Grade Count:68 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Charpy Impact, Notched | 0.100 - 4.80 J/cm² @Temperature -40.0 - 0.000 °C |
0.476 - 22.8 ft-lb/in² @Temperature -40.0 - 32.0 °F |
Average value: 0.394 J/cm² Grade Count:108 |
Overview of materials for Polypropylene with 20% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Talc Filler".Specific grades with primary filler content between 15% and 24% are .. |
|||
Charpy Impact, Notched | 0.100 - 1.80 J/cm² | 0.476 - 8.57 ft-lb/in² | Average value: 0.707 J/cm² Grade Count:60 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Charpy Impact, Notched | 0.100 - 1000 J/cm² | 0.476 - 4760 ft-lb/in² | Average value: 1.21 J/cm² Grade Count:161 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | |
LATI Laticonther 52/11 CP1/600 F3 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Potentially suitable for food/medical contact application.Availability: Africa & Middle East; Asia Pacific.. |
|||
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | |
LATI Laticonther 52/11 CP3/600 F3 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Potentially suitable for food/medical contact application.Availability: Africa & Middle East; Asia Pacific.. |
|||
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | |
LATI Latilub 57-10T Y/15 PPA, Aramid Reinforced Self-lubricating product based on Semi-aromatic polyamide (PPA). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature 23.0 °C |
0.476 ft-lb/in² @Temperature 73.4 °F |
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Asia Pacific) Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -20.0 °C |
0.476 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Daploy™ WB130HMS High Melt Strength Polypropylene for Foam Extrusion Daploy WB130HMS resin is a propylene-based, structurally isomeric polymer, which combines significantly increased melt strength with largely drawability of the polymer melt. Thus, the material is g.. |
|||
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | ISO Data, Low Temp |
Dow Tyril® 125 SAN Dow TYRIL® 125 resin is specially formulated for blending and is an ideal carrier material for use in making color concentrates. It offers high melt flow and excellent chemical resistance.Data prov.. |
|||
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | DIN 53453 |
3A Composites Core Materials AIREX® R82.60 High Performance Structural Foam AIREX® R82 is a closed-cell, thermoplastic polymer foam that combines fire resistance with low smoke and toxicity, along with good dielectric properties. It has a good strength to weight ratio, ver.. |
|||
Charpy Impact, Notched | 0.100 - 1.20 J/cm² @Temperature -30.0 - -20.0 °C |
0.476 - 5.71 ft-lb/in² @Temperature -22.0 - -4.00 °F |
Average value: 0.500 J/cm² Grade Count:5 |
Overview of materials for Nylon 66, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are inclu.. |
|||
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | 80*10*4mm, Cut; ISO 179/1eA |
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1030 PP SABIC® PPcompound 19T1030 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding applications... |
|||
Charpy Impact, Notched | 0.100 J/cm² @Temperature -30.0 °C |
0.476 ft-lb/in² @Temperature -22.0 °F |
80*10*4mm, Cut; ISO 179/1eA |
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1030 PP SABIC® PPcompound 19T1030 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding applications... |
|||
Charpy Impact, Notched | 0.100 - 0.600 J/cm² @Temperature -40.0 - -20.0 °C |
0.476 - 2.86 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 0.193 J/cm² Grade Count:46 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Charpy Impact, Notched | 0.100 J/cm² | 0.476 ft-lb/in² | |
LATI Latimass 37 B01-01 D025 Bio-Polymer Specific density compound based on Bio-Polymer (PLA, PHB, ...). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind.. |
|||
Charpy Impact, Notched | 0.100 - 2.20 J/cm² | 0.476 - 10.5 ft-lb/in² | Average value: 0.924 J/cm² Grade Count:39 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Charpy Impact, Notched | 0.100 - 12.0 J/cm² @Temperature -30.0 - 0.000 °C |
0.476 - 57.1 ft-lb/in² @Temperature -22.0 - 32.0 °F |
Average value: 1.91 J/cm² Grade Count:27 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |
|||
Charpy Impact, Notched | 0.100 - 2.90 J/cm² @Temperature -40.0 - -20.0 °C |
0.476 - 13.8 ft-lb/in² @Temperature -40.0 - -4.00 °F |
Average value: 1.28 J/cm² Grade Count:69 |
Overview of materials for Polypropylene with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are i.. |
|||
Charpy Impact, Notched | 0.100 - 0.100 J/cm² @Temperature -20.0 - -20.0 °C |
0.476 - 0.476 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 0.100 J/cm² Grade Count:1 |
Overview of materials for Polypropylene with 40% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Mica Filler". Specific grades with primary filler content between 35% and 44% are.. |