Mechanical Properties Metric English Comments
Ball Indentation Hardness 36.0 MPa
5220 psi
ISO 2039-1
Quadrant EPP Cestilene™ HD 1000 Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Ball Indentation Hardness 36.0 - 60.0 MPa
5220 - 8700 psi
Average value: 48.6 MPa Grade Count:10
Overview of materials for Polytetrafluoroethylene (PTFE), Bronze Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Bronze Filled". Each property range of values reported is minimum and ma..
Ball Indentation Hardness 36.0 MPa
5220 psi
30 sec
Mikro-Technik Mikrolen UHMW-PE
Properties: very good impact resistance / high absorption at shock and impact stress extremely high resistance against abrasive wear good corrosion resistance highly resistant at temperatures of -26..
Ball Indentation Hardness 36.0 MPa
5220 psi
Hc 30; ISO 2039; partially
Schwartz Technical Plastics LAMIGAMID® 710 High Density Polyethylene
Application: chain-guides, cutting plates, linersInformation provided by Schwartz Technical Plastics GmbH
Ball Indentation Hardness 36.0 MPa
5220 psi
ISO 2039
Borealis Borcom™ WE007AE Polypropylene
Borcom™ WE007AE is a polypropylene microcomposite intended for injection molding. The product is available in natural color. This material has an excellent balance between impact strength and stif..
Ball Indentation Hardness 36.0 MPa
5220 psi
132N/10s; ISO 2039
Borealis EE002AE Polypropylene Elastomer Modified
EE002AE is a reactor elastomer modified polypropylene compound intended for injection molding. The product is available in natural color. This material has excellent balanced mechanical properties..
Ball Indentation Hardness 36.0 MPa
5220 psi
DIN 2039
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy
Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato..
Ball Indentation Hardness 36.0 MPa
5220 psi
ISO 2039-1
Azoty Tarnow™ TARFLEN SM-B30 PTFE
Reinforced with 30% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.