Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Azoty Tarnow™ TARFLEN SM-B30 PTFE

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Bronze Filled
Manufacturer Azoty Tarnow™ (Zaklady Azotowe)
Trade Name TARFLEN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Azoty Tarnow™ TARFLEN SM-B30 PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Reinforced with 30% bronze for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Physical Properties Metric English Comments
Density 2.80 g/cc
0.101 lb/in³
ISO 1183
Filler Content 30 %
30 %
Bronze Filler
Particle Size 40 µm
40 µm
Average
Mechanical Properties Metric English Comments
Hardness, Shore D 58
58
ISO 868
Ball Indentation Hardness 36.0 MPa
5220 psi
ISO 2039-1
Tensile Strength, Yield 20.0 MPa
2900 psi
ISO 527
Elongation at Break 310 %
310 %
ISO 527
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ISO 180
Thermal Properties Metric English Comments
CTE, linear 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ASTM E 831
Melting Point 327 °C
621 °F
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Processing Temperature 360 °C
680 °F
Molding
Back Pressure 40.0 - 60.0 MPa
5800 - 8700 psi
Molding Pressure