Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 185 MPa | 26800 psi | ISO 2039-1 |
Nilit FRIANYL A63 CV-CM 0830 9005/Z Powder-coatable nylon 6.6 for injection molding, 8% carbon fiber reinforced, 30% ceramic filled Powder-coatable nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 185 MPa | 26800 psi | ISO 2039-1 |
Nilit FRIANYL A63 GV40 Nylon 6.6 for injection molding, 40% glass fiber reinforced Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 185 MPa | 26800 psi | ISO 2039-1 |
Nilit FRIANYL C73 GV40 Nylon 6.6/6 for injection molding, 40% glass fiber reinforced Nylon 6.6/6 for injection molding, medium viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 185 MPa | 26800 psi | ISO 2039-1 |
Lanxess Durethan® BG 30 X H3.0 000000 Nylon 6, 30% Glass Fibers/Glass Spheres PA 6, 30% glass fibers/glass spheres, injection molding, heat-ageing stabilized, low tendency to warp |
|||
Ball Indentation Hardness | 185 MPa | 26800 psi | ISO 2039-1 |
Lanxess Durethan® BG 30 X W1 000000 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers/glass spheres, injection molding, low tendency to warp, weather stabilizedInformation provided by LANXESS. |
|||
Ball Indentation Hardness | 185 MPa | 26800 psi | ISO 2039-1 (H 961-30) |
Lucite International Diakon® CMG302 Acrylic Polymer Information provided by Lucite International |
|||
Ball Indentation Hardness | 185 MPa | 26800 psi | ISO 2039-1 |
Lucite International Diakon® CMG314V Acrylic Polymer Information provided by Lucite International |
|||
Ball Indentation Hardness | 185 MPa | 26800 psi | ISO 2039-1 (H 961-30) |
Lucite International Diakon® CMG334V Acrylic Polymer Information provided by Lucite International |
|||
Ball Indentation Hardness | 185 MPa | 26800 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® BG-25 S PA6-GF25 Product description: Grilon BG-25 S is a heat stabilized PA6 injection molding grade with 25 % glass fibers. Grilon BG-25 S has the following important properties: Excellent surface finishEasy flowi.. |
|||
Ball Indentation Hardness | 185 MPa | 26800 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® GVN-35H black 9915 PA*-GF35 Product description: Grivory GVN-35H is a 35% glass-fiber reinforced, impact-modified engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic c.. |
|||
Ball Indentation Hardness | 185 MPa | 26800 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® LV-65H FWA black 9225 PA12-GF65 Product description: Grilamid LV-65H FWA black 9225 is a 65 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combine.. |
|||
Ball Indentation Hardness | 185 MPa | 26800 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® LV-65H FWA nat PA12-GF65 Product description: Grilamid LV-65H FWA natural is a 65 % glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following special features: High stiffness combined w.. |
|||
Ball Indentation Hardness | 185 MPa | 26800 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSGL-40/4 black 9833 PA666-GF40 Product description: Grilon TSGL-40/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 black is characterized by the following key-p.. |
|||
Ball Indentation Hardness | 185 MPa | 26800 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSGL-40/4 FA black 9840 PA666-GF40 Product description: Grilon TSGL-40/4 FA black 9840 is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 FA black 9840 is characterized by th.. |
|||
Ball Indentation Hardness | 185 MPa | 26800 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® XE 4106 black 9992 PA612-GF30 Product description: Grilamid XE 4106 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorpti.. |
|||
Ball Indentation Hardness | 185 MPa | 26800 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® XE 4106 nat PA612-GF30 Product description: Grilamid XE 4106 natural is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorptiong.. |
|||
Ball Indentation Hardness | 185 MPa | 26800 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 4176 black 9288 PA1010-GF50 Product description: Grilamid XE 4176 black 9288 is a 50% glass fiber reinforced, heat stabilized polyamide 1010 injection molding grade. The main features of Grilamid XE 4176 black 9288 are: PA1010.. |
|||
Ball Indentation Hardness | 185 MPa @Load 36.5 kg |
26800 psi @Load 80.5 lb |
dry; ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 GF15 Polyamide 6 - Glass Fiber Reinforced 15% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |