Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 135 MPa | 19600 psi | ISO 2039-1 |
Polycasa XT 620 PMMA QUINN XT sheets have good optical properties and a brilliant surface. QUINN XT sheets offer excellent transparency, good mechanical properties, are UV resistant, have very good weathering and ageing.. |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | ISO 2039-1 |
Nilit FRIANYL B63 F Raw extruded nylon 6 for injection molding Raw extruded nylon 6 for injection molding, highly crystallized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | ISO 2039-1 |
Nilit FRIANYL B63 HS-SG-GV2010 Nylon 6 for injection molding, 20% mineral filled, 10% glass fiber reinforced Nylon 6 for injection molding, high impact modified.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | ISO 2039-1 |
Nilit FRIANYL B63 UF Nylon 6 for injection molding Nylon 6 for injection molding, highly crystallized, UV stabilizedInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | ISO 2039-1 |
Nilit FRIANYL B63 V2 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | ISO 2039-1 |
Nilit FRIANYL B63 W Nylon 6 for injection molding Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | ISO 2039-1 |
Nilit FRIANYL A63 HS-GV40 Nylon 6.6 for injection molding, 40% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | ISO 2039-1 |
Nilit FRIANYL B63 H Nylon 6 for injection molding Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | ISO 2039-1 |
Nilit FRIANYL B63 HH Nylon 6 for injection molding Nylon 6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | ISO 2039-1 |
Nilit FRIANYL B63 H-SG40 Nylon 6 for injection molding, 40% mineral filled Nylon 6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | ISO 2039-1 |
Nilit FRIANYL B63 V0 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant, free of halogen and phosphorus.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | ISO 2039-1 |
Nilit RECONYL A Recycled nylon 6.6 for injection molding Recycled nylon 6.6 for injection molding (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | Hc 30; ISO 2039; partially |
Schwartz Technical Plastics LAMIGAMID® 600 Polyoxymethylene Application: friction bearings, wear and sliding linersInformation provided by Schwartz Technical Plastics GmbH |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | DIN 53456 |
Zell-Metall Engineering Plastics Zellamid 1100 OIL Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces .. |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® EB 50 H PA6 Product description: Grilon EB 50 H is a high viscosity, unreinforced, heat stabilized PA6 extrusion blow mounding grade. Grilon EB 50 H has the following important properties: High melt strengthImp.. |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSGK-30/4 X PA666-(GF+GB)30 Product description: Grilon TSGK-30 X/4 is a heat stabilized PA 66 + PA 6 injection molding grade with a 30% reinforcement combination (glass fibers and glass beads). Grilon TSGK-30/4 X has the foll.. |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® TSM-30/4 PA666-MD30 Information provided by EMS Grivory |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSS PA666 Product description: Grilon TSS is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS has the following important properties: Excellent flow behaviorHi.. |
|||
Ball Indentation Hardness | 135 MPa @Load 36.5 kg |
19600 psi @Load 80.5 lb |
ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 MCS I8 Polyamide 6 - Impact Modified Increased impact resistance grade. Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main propert.. |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | 358 N; ISO 2039-1 |
Azoty Tarnow™ TARNOFORM 500 LS POM High flow injection molding grade based on Tarnoform 500 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | 358 N; ISO 2039-1 |
Azoty Tarnow™ TARNOFORM 500 POM Easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | 358 N; ISO 2039-1 |
Azoty Tarnow™ TARNOFORM 700 POM Easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Ball Indentation Hardness | 135 MPa @Load 36.5 kg, Time 30.0 sec |
19600 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® N2320 006 POM Description: Is a POM, high-molecular-weight grade with somewhat increased flowability for injection molding of relatively thick-walled moldings.Information provided by BASF |
|||
Ball Indentation Hardness | 135 MPa @Load 36.5 kg, Time 30.0 sec |
19600 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® W2320 U035 LEV POM Description: Is a POM, UV-stabilized, very free-flowing, rapidly solidifying grade for injection molding, with reduced emission potential.Information provided by BASF |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | ISO 11359-1/-2 |
BASF Ultrason S 2010 PSU Ultrason S 2010 is an unreinforced, medium viscosity standard injection molding PSU grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req.. |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | 358 N; ISO 2039-1 |
Azoty Tarnow™ TARNOFORM 200 LS POM Injection molding grade based on Tarnoform 200 modified with soluble light stabilizers improving weathering stability.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | 358 N; ISO 2039-1 |
Azoty Tarnow™ TARNOFORM 200 POM This material is a standard extrusion grade, also could be used for injection molding of low shape complexity details.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | ISO 2039-1 |
BASF Ultrason S 3010 PSU Ultrason S 3010 is an unreinforced, higher viscosity injection molding and extrusion PSU grade, tougher and with improved chemical resistance. It conforms to FDA requirements of 21 CFR 177.1655. |
|||
Ball Indentation Hardness | 135 MPa @Load 36.5 kg, Time 30.0 sec |
19600 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultrason® S 3010 MR UN PSU Description: Unreinforced, higher viscosity injection molding and extrusion grade, tougher, with improved chemical resistance and demolding optimized. Abbreviated designation according to ISO 1043-1.. |
|||
Ball Indentation Hardness | 135 MPa | 19600 psi | ISO 2039-1 |
BASF Ultrason S 6010 PSU Ultrason S 6010 is an unreinforced, high molecular weight injection-molding and extrusion grade with excellent chemical resistance (stress crack resistance) and good solubility in typical solvents (.. |